Complete Set of CAMPUSĀ® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Alfater - TPV - MOCOM Compounds GmbH & Co. KG

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Alfater" in Material Data Center leads to the following information:

Tradename: Alfater
Family: TPV
Producer: MOCOM Compounds GmbH & Co. KG
57 hits in the material database
4 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
ALFATER XL A35I 2GP0050 TPV
ALFATER XL A40I 2GP0050 TPV
ALFATER XL A60E 2GP0000 TPV
ALFATER XL A60I 2GP0050 TPV
ALFATER XL A65E 2GP0000 TPV
ALFATER XL A70I 2GP0050 TPV
ALFATER XL A80I 2GP0050 TPV
ALFATER XL A85E 2GP0000 TPV
ALFATER XL A90E 2GP0000 TPV
ALFATER XL A90I 2GP0050 TPV
ALFATER XL D40E 2GP0000 TPV
ALFATER XL D40I 2GP0050 TPV
ALFATER XL D50E 2GP0000 TPV
ALFATER XL D50I 2GP0050 TPV
ALFATER XL A30I 4GP0000 TPV
ALFATER XL A40I 4GP0000 TPV
ALFATER XL A50I 4GP0000 TPV
ALFATER XL A75I 4GP0000 TPV
ALFATER XL A90I 4GP0000 TPV
ALFATER XL A50I 2GP0000 TPV
ALFATER XL A65I 2GP0000 TPV
ALFATER XL A50I 3EF0010 TPV
ALFATER XL A50I 4FC0010 TPV
ALFATER XL A55I 2GP0000 TPV
ALFATER XL A55I 2GP0050 TPV
ALFATER XL A55I 4PA0010 TPV
ALFATER XL A60I 3EF0010 TPV
ALFATER XL A60I 4FC0010 TPV
ALFATER XL A70I 3EF0010 TPV
ALFATER XL A70I 4GP0000 TPV
ALFATER XL A70I 4PA0010 TPV
ALFATER XL A75I 2GP0000 TPV
ALFATER XL A75I 2GP0050 TPV
ALFATER XL A80E 2GP0000 TPV
ALFATER XL A80I 3EF0010 TPV
ALFATER XL A80I 4FC0010 TPV
ALFATER XL A85I 2GP0050 TPV
ALFATER XL A85I 4PA0010 TPV
ALFATER XL A90I 2GP0001 TPV
ALFATER XL A90I 3EF0010 TPV
ALFATER XL A90I 4FC0010 TPV
ALFATER XL D40I 3EF0010 TPV
ALFATER XL D40I 4FC0010 TPV
ALFATER XL D40I 4GP0000 TPV
ALFATER XL A40I 4FC0010 TPV
ALFATER XL A65E 2GP0000 WT1159-17 TPV
ALFATER XL A80 2EC0000 TPV
ALFATER XL ECO A75I 2GP0000 TPV
ALFATER XL ECO A75I 2GP0001 TPV
ALFATER XL ECO D40 2GP0000 TPV
ALFATER XL ECO D50I 2GP0000 TPV
ALFATER XL A40I 3EF0010 TPV
ALFATER XL A60I 2UV0000 UV TPV
ALFATER XL A65I 2GP0050 TPV
ALFATER XL A70I 3EFSL0000 TPV
ALFATER XL A80I 2FE0002 TPV
ALFATER XL D40I 2GP0000 TPV

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.