Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Apec® 2045 - PC - Covestro Deutschland AG

Material Data Center offers the following functions for Apec® 2045:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Apec datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 8 cm³/10min ISO 1133
Temperature 330 °C -
Load 2.16 kg -
Melt flow index, MFI 8 g/10min ISO 1133
Temperature 330 °C -
Load 2.16 kg -
Molding shrinkage, parallel 1.1 % ISO 294-4, 2577
Molding shrinkage, normal 1.1 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2400 MPa ISO 527
Yield stress 75 MPa ISO 527
Yield strain 6.8 % ISO 527
Nominal strain at break >50 % ISO 527
Flexural modulus, 23°C 2450 MPa ISO 178
Flexural strength 110 MPa ISO 178
Charpy impact strength, +23°C N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C N kJ/m² ISO 179/1eU
Puncture - maximum force, +23°C 5000 N ISO 6603-2
Puncture - maximum force, -30°C 5500 N ISO 6603-2
Puncture energy, +23°C 50 J ISO 6603-2
Puncture energy, -30°C 58 J ISO 6603-2
Ball indentation hardness 130 MPa ISO 2039-1
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 173 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 192 °C ISO 75-1/-2
Vicat softening temperature, B 203 °C ISO 306
Coeff. of linear therm. expansion, parallel 65 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 65 E-6/K ISO 11359-1/-2
Burning behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm -
Burning behav. at thickness h HB class IEC 60695-11-10
Thickness tested 3.0 mm -
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 100Hz 2.9 - IEC 62631-2-1
Relative permittivity, 1MHz 2.8 - IEC 62631-2-1
Dissipation factor, 100Hz 10 E-4 IEC 62631-2-1
Dissipation factor, 1MHz 90 E-4 IEC 62631-2-1
Volume resistivity 1E15 Ohm*m IEC 62631-3-1
Surface resistivity 1E16 Ohm IEC 62631-3-2
Electric strength 35 kV/mm IEC 60243-1
Optical propertiesValueUnitTest Standard
ISO Data
Luminous transmittance 90[1] % ISO 13468-1, -2
Other Standards[S]
Index of Refraction 1.57 - ISO 489
1: 1 mm  S: These properties are reported by the producer according standards that are different to our defaults.
Other propertiesValueUnitTest Standard
Water absorption 0.3 % Sim. to ISO 62
Humidity absorption 0.12 % Sim. to ISO 62
Density 1130 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 330 °C ISO 294
Injection Molding, mold temperature 100 °C ISO 294
Injection Molding, injection velocity 200 mm/s ISO 294
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 130 °C -
Pre-drying - Time 2 - 3 h -
Processing humidity ≤0.02 % -
Melt temperature 330 - 340 °C -
Mold temperature 130 - 150 °C -
Zone 1 295 - 305 °C -
Zone 2 305 - 315 °C -
Zone 3 315 - 325 °C -
Nozzle temperature 325 - 335 °C -
Back pressure 5 - 15 MPa -
Characteristics
Processing
Injection Molding
Additives
Release agent
Special Characteristics
Heat stabilized or stable to heat, Sterilizable, Steam sterilization
Certifications
Medical Grade, Biocompatibility ISO 10993, US Pharmacopeia Class VI Approved
Applications
Medical
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.