Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Bayblend® FR3021 - (PC+ABS)-T15 FR(40) - Covestro Deutschland AG

Material Data Center offers the following functions for Bayblend® FR3021:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Bayblend datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
  • (PC ABS)-Blend
  • 15 % mineral filled
  • flame retardant
  • Vicat/B 120 temperature = 98 °C
  • high stiffness
  • tensile modulus = 4800 MPa
  • UL recognition 94 V-0 at 1.5 mm
  • glow wire temperature (GWFI): 960 °C at 2.0 mm
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 13 cm³/10min ISO 1133
Temperature 240 °C -
Load 5 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 4800 MPa ISO 527
Yield stress 65 MPa ISO 527
Yield strain 3 % ISO 527
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 85 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 92 °C ISO 75-1/-2
Vicat softening temperature, B 96 °C ISO 306
Coeff. of linear therm. expansion, parallel 46 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 63 E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. V-0 class IEC 60695-11-10
Thickness tested 1.5 mm -
Burning Behav. at thickness h V-0 class IEC 60695-11-10
Thickness tested 1.2 mm -
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 100Hz 3.1 - IEC 62631-2-1
Relative permittivity, 1MHz 3 - IEC 62631-2-1
Dissipation factor, 100Hz 50 E-4 IEC 62631-2-1
Dissipation factor, 1MHz 70 E-4 IEC 62631-2-1
Volume resistivity >1E13 Ohm*m IEC 62631-3-1
Surface resistivity >1E15 Ohm IEC 62631-3-2
Electric strength 35 kV/mm IEC 60243-1
Comparative tracking index 275 - IEC 60112
Other propertiesValueUnitTest Standard
Water absorption 0.5 % Sim. to ISO 62
Humidity absorption 0.2 % Sim. to ISO 62
Density 1280 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 240 °C ISO 294
Injection Molding, mold temperature 80 °C ISO 294
Injection Molding, injection velocity 240 mm/s ISO 294
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 75 - 100 °C -
Pre-drying - Time 2 - 4 h -
Processing humidity ≤0.02 % -
Melt temperature 240 - 280 °C -
Mold temperature 70 - 100 °C -
Diagrams
Viscosity-shear rate , Bayblend® FR3021, (PC+ABS)-T15 FR(40), Covestro
Shearstress-shear rate , Bayblend® FR3021, (PC+ABS)-T15 FR(40), Covestro
Dynamic Shear modulus-temperature , Bayblend® FR3021, (PC+ABS)-T15 FR(40), Covestro
Stress-strain , Bayblend® FR3021, (PC+ABS)-T15 FR(40), Covestro
Secant modulus-strain , Bayblend® FR3021, (PC+ABS)-T15 FR(40), Covestro
Stress-strain (isochronous) 23°C, Bayblend® FR3021, (PC+ABS)-T15 FR(40), Covestro
Creep modulus-time 23°C, Bayblend® FR3021, (PC+ABS)-T15 FR(40), Covestro
Creep curve 23°C, Bayblend® FR3021, (PC+ABS)-T15 FR(40), Covestro
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Release agent
Special Characteristics
Flame retardant
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Other text information
Injection molding
PREPROCESSING
Max. Water content: 0.02 %
Drying temperature: 75 - 100 °C
(depending on the grade 10°C below the Vicat VST/B120 temperature, but not higher as the recommended values).
Drying time:
Circulating air drying oven (50 % fresh air) 4-8 h
Fresh air dryer (high speed dryer) 2-4 h
Dry air dryer 2-4 h

PROCESSING
Melt temperature: 240-280 °C
Mold temperature: 70-100 °C

Use open nozzle.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.