Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Bayblend® T85 X RE - (PC+ABS) - Covestro Deutschland AG

Material Data Center offers the following functions for Bayblend® T85 X RE:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Bayblend datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
  • (PC+ABS)-Blend
  • General Purpose Grade
  • Vicat/B 120 temperature = 131 °C
  • good injection molding processing behaviour (easy flowing)
  • excellent long-term ageing behaviour under humid conditions and painting performance
  • improved chemical resistance
  • low VOC emissions and odour
Partially bio-circular grade / Attributed via mass balance (according to ISCC PLUS Standard).
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 18 cm³/10min ISO 1133
Temperature 260 °C -
Load 5 kg -
Molding shrinkage, parallel 0.8 % ISO 294-4, 2577
Molding shrinkage, normal 0.8 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2300 MPa ISO 527
Yield stress 56 MPa ISO 527
Yield strain 4.9 % ISO 527
Nominal strain at break >50 % ISO 527
Charpy impact strength, +23°C N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C N kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 60 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 47 kJ/m² ISO 179/1eA
Izod impact strength, +23°C N kJ/m² ISO 180/1U
Izod notched impact strength, +23°C 57 kJ/m² ISO 180/1A
Izod notched impact strength 46 kJ/m² ISO 180/1A
Temperature -30 °C -
Puncture - maximum force, +23°C 4500 N ISO 6603-2
Puncture - maximum force, -30°C 5400 N ISO 6603-2
Puncture energy, +23°C 48 J ISO 6603-2
Puncture energy, -30°C 56 J ISO 6603-2
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 106 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 127 °C ISO 75-1/-2
Vicat softening temperature, B 129 °C ISO 306
Coeff. of linear therm. expansion, parallel 70 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 70 E-6/K ISO 11359-1/-2
Burning Behav. at thickness h HB class IEC 60695-11-10
Thickness tested 0.8 mm -
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 100Hz 3 - IEC 62631-2-1
Relative permittivity, 1MHz 3 - IEC 62631-2-1
Dissipation factor, 100Hz 20 E-4 IEC 62631-2-1
Dissipation factor, 1MHz 90 E-4 IEC 62631-2-1
Volume resistivity >1E13 Ohm*m IEC 62631-3-1
Surface resistivity >1E15 Ohm IEC 62631-3-2
Electric strength 40 kV/mm IEC 60243-1
Comparative tracking index 225 - IEC 60112
Other propertiesValueUnitTest Standard
Water absorption 0.4 % Sim. to ISO 62
Humidity absorption 0.1 % Sim. to ISO 62
Density 1140 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 280 °C ISO 294
Injection Molding, mold temperature 80 °C ISO 294
Injection Molding, injection velocity 240 mm/s ISO 294
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 95 - 110 °C -
Pre-drying - Time 4 h -
Processing humidity ≤0.01 % -
Melt temperature 270 - 290 °C -
Mold temperature 70 - 90 °C -
Characteristics
Processing
Injection Molding
Features
Low Emission, Low Odor
Chemical Resistance
General Chemical Resistance
Certifications
Contains renewable resources, ISCC Plus
Applications
General Purpose
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.