Any use of this information falls under the rules of our
disclaimer.
Processing/Physical Characteristics | Value | Unit | Test Standard |
ISO Data |
Melt flow index, MFI |
15 |
g/10min |
ISO 1133 |
Temperature |
300 |
°C |
- |
Load |
1.2 |
kg |
- |
Molding shrinkage, parallel |
0.6 |
% |
ISO 294-4, 2577 |
ASTM Data |
Melt Flow Index, MFI |
15 |
g/10min |
ASTM D 1238 |
Temperature |
300 |
°C |
- |
Load |
1.2 |
kg |
- |
Mold Shrinkage, MD |
0.006 |
mm/mm |
ASTM D 955 |
Mechanical properties | Value | Unit | Test Standard |
ISO Data |
Tensile Modulus |
2300 |
MPa |
ISO 527 |
Yield stress |
62 |
MPa |
ISO 527 |
Yield strain |
6 |
% |
ISO 527 |
Stress at break |
68 |
MPa |
ISO 527 |
Strain at break |
130 |
% |
ISO 527 |
Flexural modulus, 23°C |
2400 |
MPa |
ISO 178 |
Flexural strength |
97 |
MPa |
ISO 178 |
Charpy notched impact strength, +23°C |
25 |
kJ/m² |
ISO 179/1eA |
Izod notched impact strength, +23°C |
75 |
kJ/m² |
ISO 180/1A |
ASTM Data |
Tensile Modulus |
2206 |
MPa |
ASTM D 638 |
Tensile Strength at Yield |
62.1 |
MPa |
ASTM D 638 |
Tensile Strength at Break |
68.3 |
MPa |
ASTM D 638 |
Elongation at Yield |
6 |
% |
ASTM D 638 |
Elongation at Break |
130 |
% |
ASTM D 638 |
Flexural Modulus |
2413 |
MPa |
ASTM D 790 |
Flexural Strength |
96.5 |
MPa |
ASTM D 790 |
Rockwell Hardness |
R 118 |
- |
ASTM D 785 |
Izod Impact notched, 1/8 in |
747 |
J/m |
ASTM D 256 |
Thermal properties | Value | Unit | Test Standard |
ISO Data |
Temp. of deflection under load, 1.80 MPa |
120 |
°C |
ISO 75-1/-2 |
Vicat softening temperature, B |
138 |
°C |
ISO 306 |
ASTM Data |
Coefficient of Thermal Expansion, MD |
68.4 |
E-6/K |
ASTM D 696 |
DTUL @ 66 psi |
139[ann.] |
°C |
ASTM D 648 |
DTUL @ 264 psi |
122 |
°C |
ASTM D 648 |
Vicat Temperature |
143 |
°C |
ASTM D 1525 |
Electrical properties | Value | Unit | Test Standard |
ISO Data |
Electric strength |
17 |
kV/mm |
IEC 60243-1 |
ASTM Data |
Dielectric Strength, Short Time |
16.5 |
kV/mm |
ASTM D 149 |
Dissipation Factor, 1 MHz |
0.002 |
- |
ASTM D 150 |
Dielectric Constant, 60 Hz |
3 |
- |
ASTM D 150 |
Dielectric Constant, 1 MHz |
3 |
- |
ASTM D 150 |
Volume Resistivity |
2E17 |
Ohm*cm |
ASTM D 257 |
Optical properties | Value | Unit | Test Standard |
ASTM Data |
Haze |
2 |
% |
ASTM D 1003 |
Light Transmittance |
85 |
% |
ASTM D 1003 |
Index of Refraction |
1.59 |
- |
ASTM D 542 |
Other properties | Value | Unit | Test Standard |
Water absorption |
0.12 |
% |
Sim. to ISO 62 |
Humidity absorption |
0.15 |
% |
Sim. to ISO 62 |
Density |
1200 |
kg/m³ |
ISO 1183 |
Water Absorption, 24hr |
0.15 |
% |
ASTM D 570 |
Density |
1200 |
kg/m³ |
ASTM D 792 |
Processing Recommendation Injection Molding | Value | Unit | Test Standard |
Pre-drying - Temperature |
120 |
°C |
- |
Pre-drying - Time |
4 |
h |
- |
Melt temperature |
275 - 295 |
°C |
- |
Mold temperature |
70 - 90 |
°C |
- |
Characteristics
Processing
Injection Molding
Additives
Release agent
Special Characteristics
Transparent, Sterilizable, Gamma irradiation sterilization, Electron beam (e-beam) sterilization
Chemical Resistance
Radiation Resistance
Certifications
Medical Grade, Biocompatibility ISO 10993
Applications
Medical
Regional Availability
North America, Europe, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com