Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CALIBRE™ 301-EP-22 - PC - Trinseo

Material Data Center offers the following functions for CALIBRE™ 301-EP-22:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Calibre datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt flow index, MFI 22 g/10min ISO 1133
Temperature 300 °C -
Load 1.2 kg -
Molding shrinkage, parallel 0.6 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2300 MPa ISO 527
Yield stress 60 MPa ISO 527
Yield strain 6 % ISO 527
Stress at break 65 MPa ISO 527
Strain at break >50 % ISO 527
Flexural modulus, 23°C 2400 MPa ISO 178
Charpy notched impact strength, +23°C 20 kJ/m² ISO 179/1eA
Izod notched impact strength, +23°C 74 kJ/m² ISO 180/1A
Rockwell hardness R118 - ISO 2039-2
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 122 °C ISO 75-1/-2
Vicat softening temperature, B 147 °C ISO 306
Coeff. of linear therm. expansion, parallel 68 E-6/K ISO 11359-1/-2
Burning behav. at 1.5 mm nom. thickn. V-2 class IEC 60695-11-10
Thickness tested 1.5 mm -
Burning behav. at thickness h V-2 class IEC 60695-11-10
Thickness tested 3.0 mm -
Oxygen index 26 % ISO 4589-1/-2
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 100Hz 3 - IEC 62631-2-1
Relative permittivity, 1MHz 3 - IEC 62631-2-1
Dissipation factor, 1MHz 20 E-4 IEC 62631-2-1
Volume resistivity >1E13 Ohm*m IEC 62631-3-1
Electric strength 17 kV/mm IEC 60243-1
Comparative tracking index 250 - IEC 60112
Optical propertiesValueUnitTest Standard
ASTM Data
Haze 1 % ASTM D 1003
Light Transmittance 89 % ASTM D 1003
Index of Refraction 1.59 - ASTM D 542
Other propertiesValueUnitTest Standard
Humidity absorption 0.32 % Sim. to ISO 62
Density 1200 kg/m³ ISO 1183
Characteristics
Processing
Injection Molding
Additives
Release agent
Special Characteristics
High impact or impact modified, Heat stabilized or stable to heat
Applications
Electrical and Electronical
Regional Availability
North America, Europe, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.