Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CALIBRE™ MEGARAD™ 2081-15 - PC - Trinseo

Material Data Center offers the following functions for CALIBRE™ MEGARAD™ 2081-15:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Calibre datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt flow index, MFI 15 g/10min ISO 1133
Temperature 300 °C -
Load 1.2 kg -
Molding shrinkage, parallel 0.6 % ISO 294-4, 2577
ASTM Data
Melt Flow Index, MFI 15 g/10min ASTM D 1238
Temperature 300 °C -
Load 1.2 kg -
Mold Shrinkage, MD 0.006 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2300 MPa ISO 527
Yield stress 62 MPa ISO 527
Yield strain 6 % ISO 527
Stress at break 68 MPa ISO 527
Strain at break 130 % ISO 527
Flexural modulus, 23°C 2400 MPa ISO 178
Flexural strength 97 MPa ISO 178
Charpy notched impact strength, +23°C 25 kJ/m² ISO 179/1eA
Izod notched impact strength, +23°C 75 kJ/m² ISO 180/1A
ASTM Data
Tensile Modulus 2206 MPa ASTM D 638
Tensile Strength at Yield 62.1 MPa ASTM D 638
Tensile Strength at Break 68.3 MPa ASTM D 638
Elongation at Yield 6 % ASTM D 638
Elongation at Break 130 % ASTM D 638
Flexural Modulus 2413 MPa ASTM D 790
Flexural Strength 96.5 MPa ASTM D 790
Rockwell Hardness R 118 - ASTM D 785
Izod Impact notched, 1/8 in 747 J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 120 °C ISO 75-1/-2
Vicat softening temperature, B 138 °C ISO 306
ASTM Data
Coefficient of Thermal Expansion, MD 68.4 E-6/K ASTM D 696
DTUL @ 66 psi 139[ann.] °C ASTM D 648
DTUL @ 264 psi 122 °C ASTM D 648
Vicat Temperature 143 °C ASTM D 1525
ann.: annealed
Electrical propertiesValueUnitTest Standard
ISO Data
Electric strength 17 kV/mm IEC 60243-1
ASTM Data
Dielectric Strength, Short Time 16.5 kV/mm ASTM D 149
Dissipation Factor, 1 MHz 0.002 - ASTM D 150
Dielectric Constant, 60 Hz 3 - ASTM D 150
Dielectric Constant, 1 MHz 3 - ASTM D 150
Volume Resistivity 2E17 Ohm*cm ASTM D 257
Optical propertiesValueUnitTest Standard
ASTM Data
Haze 2 % ASTM D 1003
Light Transmittance 85 % ASTM D 1003
Index of Refraction 1.59 - ASTM D 542
Other propertiesValueUnitTest Standard
Water absorption 0.12 % Sim. to ISO 62
Humidity absorption 0.15 % Sim. to ISO 62
Density 1200 kg/m³ ISO 1183
Water Absorption, 24hr 0.15 % ASTM D 570
Density 1200 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 120 °C -
Pre-drying - Time 4 h -
Melt temperature 275 - 295 °C -
Mold temperature 70 - 90 °C -
Diagrams
Viscosity-shear rate , CALIBRE™ MEGARAD™ 2081-15, PC, Trinseo
Shearstress-shear rate , CALIBRE™ MEGARAD™ 2081-15, PC, Trinseo
Specific volume-temperature (pvT) , CALIBRE™ MEGARAD™ 2081-15, PC, Trinseo
Characteristics
Processing
Injection Molding
Additives
Release agent
Special Characteristics
Transparent, Sterilizable, Gamma irradiation sterilization, Electron beam (e-beam) sterilization
Chemical Resistance
Radiation Resistance
Certifications
Medical Grade, Biocompatibility ISO 10993
Applications
Medical
Regional Availability
North America, Europe, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.