Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Cawiton MT930 - SEBS - Wittenburg B.V.

Material Data Center offers the following functions for Cawiton MT930:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Cawiton datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt flow index, MFI 2.7 g/10min ISO 1133
Temperature 230 °C -
Load 5 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Strength 1.5 MPa ISO 37
Strain at break 281 % ISO 37
Compression set at 70 °C, 24h 46 % ISO 815
Tear strength 13 kN/m ISO 34-1
Shore A hardness 30 - ISO 7619-1
Other Standards[S]
Stress at 100% elongation 1.1 MPa ISO 37
Stress at 300% elongation 4.5 MPa ISO 37
S: These properties are reported by the producer according standards that are different to our defaults.
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 166 °C ISO 11357-1/-3
Other propertiesValueUnitTest Standard
Density 890 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Melt temperature 180 - 240 °C -
Mold temperature 20 - 40 °C -
Feed temperature 30 - 60 °C -
Zone 1 180 - 220 °C -
Zone 2 190 - 230 °C -
Zone 3 190 - 230 °C -
Nozzle temperature 200 - 240 °C -
Characteristics
Processing
Injection Molding
Special Characteristics
Translucent, Sterilizable, Ethylene Oxide (EtO) Sterilization, Steam sterilization, Gamma irradiation sterilization
Chemical Resistance
Radiation Resistance
Certifications
Food contact, Medical Grade, Biocompatibility ISO 10993, US Pharmacopeia Class VI Approved
Applications
Medical
Regional Availability
Europe
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.