Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CELANEX® 2300 GV1/30 - PBT-GF30 - Celanese

Material Data Center offers the following functions for CELANEX® 2300 GV1/30:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Celanex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Chemical abbreviation according to ISO 1043-1: PBT Moulding compound ISO 7792- PBT, MGHR, 08-100N, GF30 Polybutylene terephthalate, 30 % glass fibre reinforced. Flammability UL 94 HB minimum thickness 1.2 mm. Recognition by Underwriters Laboratories, USA (UL)

Flammability @3.2mm nom. thickn.HB-
Flammability @1.6mm nom. thickn.HB-
Flammability at thickness h (1 mm)HBUL recognition (h)
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 9 cm³/10min ISO 1133
Temperature 250 °C -
Load 2.16 kg -
Molding shrinkage, parallel 0.3 % ISO 294-4, 2577
Molding shrinkage, normal 1.1 % ISO 294-4, 2577
Density of melt 1320 kg/m³ -
Thermal conductivity of melt 0.166 W/(m K) -
Spec. heat capacity of melt 1720 J/(kg K) -
Ejection temperature 220 °C -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 10300 MPa ISO 527
Stress at break 150 MPa ISO 527
Strain at break 2.5 % ISO 527
Charpy impact strength, +23°C 60 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 60 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 9.5 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 9 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 225 °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 210 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 225 °C ISO 75-1/-2
Vicat softening temperature, B 220 °C ISO 306
Coeff. of linear therm. expansion, parallel 25 E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm -
Burning Behav. at thickness h HB class IEC 60695-11-10
Thickness tested 1.0 mm -
Yellow Card available yes - -
Oxygen index 20 % ISO 4589-1/-2
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 100Hz 4.4 - IEC 62631-2-1
Relative permittivity, 1MHz 4.3 - IEC 62631-2-1
Dissipation factor, 100Hz 20 E-4 IEC 62631-2-1
Dissipation factor, 1MHz 190 E-4 IEC 62631-2-1
Volume resistivity >1E13 Ohm*m IEC 62631-3-1
Surface resistivity >1E15 Ohm IEC 62631-3-2
Electric strength 33 kV/mm IEC 60243-1
Other propertiesValueUnitTest Standard
Water absorption 0.4 % Sim. to ISO 62
Humidity absorption 0.15 % Sim. to ISO 62
Density 1550 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 120 - 140 °C -
Pre-drying - Time 2 - 4 h -
Processing humidity ≤0.02 % -
Melt temperature 260 - 270 °C -
Mold temperature 75 - 85 °C -
Diagrams
Viscosity-shear rate , CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Shearstress-shear rate , CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Dynamic Shear modulus-temperature , CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Stress-strain , CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Secant modulus-strain , CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Stress-strain (isochronous) 100°C, CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Creep modulus-time 100°C, CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Creep curve 100°C, CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Stress-strain (isochronous) 23°C, CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Creep modulus-time 23°C, CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Creep curve 23°C, CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Stress-strain (isochronous) 60°C, CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Creep modulus-time 60°C, CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Creep curve 60°C, CELANEX® 2300 GV1/30, PBT-GF30, Celanese
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Release agent
Special Characteristics
Heat stabilized or stable to heat
Regional Availability
North America, Europe
Other text information
Injection molding
To avoid hydrolytic degradation during processing, CELANEX resins have to be dried to a moisture level equal to or less than 0,02%. The drying should be done in a dry-air dryer (dew point < -30°C) with a temperature of 120 to 140 °C and a drying time of 2 to 4 hours. In case of longer residence times in the dry-air dryer, the temperature should be reduced to 100°C.
The time between drying and processing should be kept as short as possible. The processing machine feed hopper should be closed during the processing operation.
Melt Temperature 260-270 °C
Mold Temperature *) 75-85 °C
Maximum Barrel Residence Time **) 5-10 min
Injection Speed fast
Peripheral screw speed max.0,3 m/sec
Back Pressure 10-30 bar
Injection Pressure 600-1000 bar
Holding Pressure 400-800 bar
Nozzle Design open design preferred

Injection speed, injection pressure and holding pressure have to be optimized to the individual article geometry. To avoid material degradation during processing low back pressure and minimum screw speed have to be used. Overheating of the material has to be avoided. For grades containing flame retardants, a maximum temperature of 265 °C should not be exceeded. Up to 25% clean and dry regrind may be used.

Celanese recommends only externally heated hot runner systems.

*) For moulded parts with especially high requirements to the surface quality or dimensional stability, a mold temperature of up to 110 °C can be advantageous.

**) If the cylinder temperatures are higher than the recommended maximum temperatures, the max. residence time in the barrel has to be reduced.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.