Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CELANEX® 5206HG - PET-GF15 - Celanese

Material Data Center offers the following functions for CELANEX® 5206HG:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Celanex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Celanex 5206HG is a 15% glass-filled polyester featuring super high surface gloss and high flow for long flow channels. A typical application is oven handles.

Flammability at thickness h (0.8 mm)HB-
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Molding shrinkage, parallel 0.5 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 6400 MPa ISO 527
Stress at break 95 MPa ISO 527
Strain at break 1.8 % ISO 527
Charpy notched impact strength, +23°C 4.7 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 250 °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 180 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 220 °C ISO 75-1/-2
Burning Behav. at thickness h HB class IEC 60695-11-10
Thickness tested 0.8 mm -
Other propertiesValueUnitTest Standard
Density 1450 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Melt temperature 270 - 300 °C -
Mold temperature 120 - 135 °C -
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Features
High Gloss
Other text information
Injection molding
Rear Temperature 480-500 (250-260) deg F (deg C)
Center Temperature 490-510 (255-265) deg F (deg C)
Front Temperature 500-540 (260-270) deg F (deg C)
Nozzle Temperature 510-520 (265-275) deg F (deg C)
Melt Temperature 520-570 (270-300) deg F (deg C)
Mold Temperature 250-275 (120-135) deg F (deg C)
Back Pressure 0-25 psi
Screw Speed 50-75 rpm
Injection Speed Medium/Fast

Injection speed, injection pressure and holding pressure have to be optimized to the individual article geometry. To avoid material degradation during processing low back pressure and minimum screw speed have to be used. Overheating of the material has to be avoided. Up to 25% clean and dry regrind may be used.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.