Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CELANEX® XFR 6842 GF30 - PBT-GF30 - Celanese

Material Data Center offers the following functions for CELANEX® XFR 6842 GF30:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Celanex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Celanex XFR 6842 GF30 is a halogen and antimony free flame retardant (V-0 @ 0.4 mm) 30% glass reinforced PBT grade with good processability and no corrosive emissions during processing. It is suitable for parts requiring enhanced tracking resistance, toughness, and flame retardancy at < 0.75 mm wall thickness and It is well suited for electrical connector applications where its UL approved 50% regrind use capability allows maximum use of purchased product.. The product is WEEE and RoHS compliant.

Flammability @1.6mm nom. thickn.V-0-
Flammability @0.8mm nom. thickn.V-0UL recognition (0.8)
Flammability @0.4mm nom. thickn.V-0UL recognition (0.4)
Flammability at thickness h (0.4 mm)V-0UL recognition (h)
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 18 cm³/10min ISO 1133
Temperature 250 °C -
Load 5 kg -
Molding shrinkage, parallel 0.4 % ISO 294-4, 2577
Molding shrinkage, normal 0.9 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 10000 MPa ISO 527
Stress at break 102 MPa ISO 527
Strain at break 2 % ISO 527
Charpy impact strength, +23°C 35 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 6.9 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 225 °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 203 °C ISO 75-1/-2
Vicat softening temperature, B 207 °C ISO 306
Burning Behav. at 1.5 mm nom. thickn. V-0 class IEC 60695-11-10
Burning Behav. at thickness h V-0 class IEC 60695-11-10
Thickness tested 0.4 mm -
Yellow Card available yes - -
Burning Behav. 5V at thickness h 5VA class IEC 60695-11-20
Thickness tested 1.5 mm -
Yellow Card available yes - -
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 1MHz 3.6 - IEC 62631-2-1
Dissipation factor, 1MHz 140 E-4 IEC 62631-2-1
Volume resistivity >1E13 Ohm*m IEC 62631-3-1
Surface resistivity >1E15 Ohm IEC 62631-3-2
Other propertiesValueUnitTest Standard
Humidity absorption 0.2 % Sim. to ISO 62
Density 1530 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 120 - 140 °C -
Pre-drying - Time 2 - 4 h -
Processing humidity ≤0.02 % -
Melt temperature 250 - 265 °C -
Mold temperature 75 - 90 °C -
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Special Characteristics
Flame retardant, Halogen-free
Features
Low Emission
Certifications
RoHS compliant
Regional Availability
North America, Europe
Other text information
Injection molding
To avoid hydrolytic degradation during processing, CELANEX resins have to be dried to a moisture level equal to or less than 0.02%. Drying should be done in a dehumidifying hopper dryer capable of dewpoints <-40°F (-40°C) at 250-285°F (120-140°C) for 4-6 hours.
Melt Temperature. 250-265 °C
Mold Temperature *): 75-90 °C
Maximum Barrel Residence Time **): 5-10 min
Injection Speed: high
Peripheral screw speed: max.0,25 m/sec
Back Pressure: 10-30 bar
Injection Pressure: 600-1000 bar
Holding Pressure: 400-800 bar

Injection speed, injection pressure and holding pressure have to be optimized to the individual article geometry. To avoid material degradation during processing low back pressure and minimum screw speed have to be used. Overheating of the material has to be avoided. For grades containing flame retardants, a maximum temperature of 265 °C should not be exceeded.

Ticona recommends only externally heated hot runner systems.

*) For moulded parts with especially high requirements to the surface quality or dimensional stability, a mold temperature of up to 100 °C can be advantageous.

**) If the cylinder temperatures are higher than the recommended maximum temperatures, the max. residence time in the barrel has to be reduced.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.