Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CirculenRenew C14 LD2420D - (PE-LD) - LyondellBasell Industries

Material Data Center offers the following functions for CirculenRenew C14 LD2420D:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Circulen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt flow index, MFI 0.25 g/10min ISO 1133
Temperature 190 °C -
Load 2.16 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 260 MPa ISO 527
Yield stress 10 MPa ISO 527
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 110 °C ISO 11357-1/-3
Vicat softening temperature, A 96 °C ISO 306
Optical propertiesValueUnitTest Standard
ASTM Data
Gloss 50 - ASTM D 2457
Haze 14 % ASTM D 1003
Other propertiesValueUnitTest Standard
Density 923 kg/m³ ISO 1183
Film PropertiesValueUnitTest Standard
ISO Data
Maximum stress, parallel 27 MPa ISO 527-3
Maximum stress, normal 25 MPa ISO 527-3
Maximum strain, parallel 200 % ISO 527-3
Maximum strain, normal 500 % ISO 527-3
Dynamic coefficient of friction 0.8 - ISO 8295
Type of extrusion blown - -
Thickness of specimen 0.05 mm -
Processing Recommendation ExtrusionValueUnitTest Standard
Type of extrusion blown - -
Melt temperature 170 - 220 °C -
Characteristics
Processing
Blown Film Extrusion, Film Extrusion
Delivery form
Pellets
Features
Melt Strength
Certifications
Contains renewable resources, Recycled Resin Content
Applications
General Purpose, Packaging
Regional Availability
Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.