Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Cosmoplene® AZ864 - PP - The Polyolefin Company (Singapore) Pte Ltd

Material Data Center offers the following functions for Cosmoplene® AZ864:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Cosmoplene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Melt Flow Index, MFI 38 g/10min ASTM D 1238
Mold Shrinkage, MD 0.015 mm/mm ASTM D 955
Mold Shrinkage, TD 0.014 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Strength at Yield 25 MPa ASTM D 638
Tensile Strength at Break 17 MPa ASTM D 638
Elongation at Break 80 % ASTM D 638
Flexural Modulus 1200 MPa ASTM D 790
Rockwell Hardness R 90 - ASTM D 785
Izod Impact notched, 1/8 in 80 J/m ASTM D 256
Izod Impact notched, Low-Temperature 42 J/m ASTM D 256
Temperature -20 °C -
Thermal propertiesValueUnitTest Standard
ASTM Data
UL 94 Flame rating HB - UL 94
DTUL @ 66 psi 122 °C ASTM D 648
Other propertiesValueUnitTest Standard
Density 900 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Mold temperature 30 °C -
Zone 1 190 - 230 °C -
Injection pressure 6.9 MPa -
Holding pressure 9.8 MPa -
Characteristics
Processing
Injection Molding
Special Characteristics
Anti-static, High impact or impact modified, U.V. stabilized or stable to weather
Features
Copolymer, Impact Copolymer
Applications
Automotive
Regional Availability
Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.