Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Cosmoplene® FL7632L - PP - The Polyolefin Company (Singapore) Pte Ltd

Material Data Center offers the following functions for Cosmoplene® FL7632L:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Cosmoplene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Melt Flow Index, MFI 7 g/10min ASTM D 1238
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Strength at Break 44 MPa ASTM D 638
Thermal propertiesValueUnitTest Standard
ASTM Data
Melting Temperature 132 °C ASTM D 3418
Optical propertiesValueUnitTest Standard
ASTM Data
Gloss 150 - ASTM D 2457
Haze 2 % ASTM D 1003
Other propertiesValueUnitTest Standard
Density 900 kg/m³ ASTM D 792
Film PropertiesValueUnitTest Standard
ASTM Data
Thickness of specimen 0.03 mm -
Other Standards[S]
Tensile Modulus, MD 420 MPa TPC Method
Tensile Modulus, TD 440 MPa TPC Method
S: These properties are reported by the producer according standards that are different to our defaults.
Characteristics
Processing
Film Extrusion
Additives
Antiblocking agent
Special Characteristics
Transparent
Features
Heat Sealable
Certifications
Food contact, Food approval FDA 21 CFR
Regional Availability
Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.