Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Cristal™ Renew 400-50 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Cristal™ Renew 400-50:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Cristal datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

Eastman Cristal™ Renew copolyester 400-50 is a high flow product. It is designed and engineered specifically for

cosmetics packaging applications. With its unsurpassed color and clarity and an unmatched ability to mold thick

parts with improved gate aesthetics, Cristal Renew 400-50 is clearly a well suited copolyester for premium

cosmetics packaging. Other outstanding features are excellent chemical resistance, high gloss, and improvements

in processing such as faster cycle times, and lower scrap rates. Cristal Renew 400-50 is also ideally suited for twoshot

molding techniques due to its lower processing temperatures, very slow crystallization rate, and flow

characteristics.

Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a

global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are

produced with ISCC certified circular content by mass balance allocation.


Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Mold Shrinkage, MD 0.0035 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2000 MPa ISO 527
Yield stress 49 MPa ISO 527
Yield strain 4.2 % ISO 527
Stress at break 21 MPa ISO 527
Strain at break 36 % ISO 527
ASTM Data
Tensile Modulus 2030 MPa ASTM D 638
Tensile Strength at Yield 50 MPa ASTM D 638
Tensile Strength at Break 25 MPa ASTM D 638
Elongation at Yield 4.4 % ASTM D 638
Elongation at Break 38 % ASTM D 638
Flexural Modulus 1810 MPa ASTM D 790
Flexural Strength 66 MPa ASTM D 790
Rockwell Hardness R 102 - ASTM D 785
Izod Impact notched, 1/8 in 104 J/m ASTM D 256
Izod Impact notched, Low-Temperature 38 J/m ASTM D 256
Temperature -40 °C -
Izod Impact unnotched, 1/8 in N J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ASTM Data
DTUL @ 66 psi 68 °C ASTM D 648
DTUL @ 264 psi 61 °C ASTM D 648
Optical propertiesValueUnitTest Standard
ASTM Data
Haze 0.24 % ASTM D 1003
Light Transmittance 91.8 % ASTM D 1003
Other propertiesValueUnitTest Standard
Density 1280 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 65 °C -
Pre-drying - Time 8 h -
Melt temperature 205 - 240 °C -
Mold temperature 16 - 38 °C -
Characteristics
Processing
Injection Molding, Other Extrusion
Special Characteristics
High impact or impact modified, Transparent
Features
High Gloss, Copolymer
Chemical Resistance
General Chemical Resistance
Certifications
ISCC Plus
Applications
Packaging
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.