Danamid - PA - Qualchem Zrt

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Danamid" in Material Data Center leads to the following information:

Tradename: Danamid
Family: PA
Producer: Qualchem Zrt
50 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
DANAMID AFCF-30 PA66-CF30
DANAMID AFCFHUV-20 PA66-CF20
DANAMID AFE PA66
DANAMID AFEHUV PA66
DANAMID AFES PA66
DANAMID AFES-21 PA66
DANAMID AFES-23 PA66
DANAMID AFGF-15 PA66-GF15
DANAMID AFGF-20 PA66-GF20
DANAMID AFGF-30 PA66-GF30
DANAMID AFGF-50 PA66-GF50
DANAMID AFGFH-30 PA66-GF30
DANAMID AFGFL0 - 20 PA6-GF20
DANAMID AFGFLPX0 - 30 PA66-GF30
DANAMID AFGFLPX0 - 35 PA66-GF35
DANAMID AFGFS2HUV14 PA66-GF14
DANAMID AFGFS2HUV30 PA66-GF30
DANAMID AFGFW10-30 PA66-(GF+MX)40
DANAMID E 1 PA6
DANAMID E 2 PA6
DANAMID FCF-20 PA6-CF20
DANAMID FCP-40 PA6-CF40
DANAMID FE PA6
DANAMID FEH PA6
DANAMID FEHUV PA6
DANAMID FEL0 PA6
DANAMID FELX0 PA6
DANAMID FES PA6
DANAMID FES-21 PA6
DANAMID FES-23 PA6
DANAMID FES-23 HUV PA6
DANAMID FEW - 10 PA6-MX10
DANAMID FEW - 25 PA6-MX25
DANAMID FEW - 30 PA6-MX30
DANAMID FEWL0 - 20 PA6-MX20
DANAMID FEWL2 - 25 PA6-MX25
DANAMID FEWLX2-25 PA6-MX25
DANAMID FGF- 10 PA6-GF10
DANAMID FGF- 15 PA6-GF15
DANAMID FGF- 20 PA6-GF20
DANAMID FGF- 30 PA6-GF30
DANAMID FGF- 50 PA6-GF50
DANAMID FGFH - 30 PA6-GF30
DANAMID FGFHUV- 30 PA6-GF30
DANAMID FGFHUVLX2 - 30 PA6-GF30
DANAMID FGFL0 - 20 PA6-GF20
DANAMID FGFL0 - 30 PA6-GF30
DANAMID FGFS- 30 PA6-GF30
DANAMID FGFS- 5 PA6-GF5
DANAMID FGFTALX2-5 20 PA6-(GF+MX)25

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.