Denilub Y - PA66 - Vamp Tech Spa
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Denilub Y" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
Datasheet | Polymer |
---|---|
Denilub Y 00U 0Mo Nat 01 | PA66-Z |
Denilub Y 00U 0Si M | (PA66+SI) |
Denilub Y 00U 10TFMo M | (PA66+PTFE)-Z |
Denilub Y 00U 23TFAr | (PA66+PTFE)-AF |
Denilub Y 15G 0Mo | PA66-(GF+Z)15 |
Denilub Y 15G 4TF | (PA66+PTFE)-GF15 |
Denilub Y 20G 4TF | (PA66+PTFE)-GF20 |
Denilub Y 30C 3TF | (PA66+PTFE)-CF30 |
Denilub Y 30G 0Mo | PA66-(GF+Z)30 |
Denilub Y 30G 3TF | (PA66+PTFE)-GF30 |
Denilub Y 50G 0Mo | PA66-(GF+Z)50 |
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.