Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Desmopan - TPU - Covestro Deutschland AG

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Desmopan" in Material Data Center leads to the following information:

Tradename: Desmopan
Family: TPU
Producer: Covestro Deutschland AG
66 hits in the material database
21 hits in the literature database
4 hits in the application database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
Desmopan 192 TPU
Desmopan® 3060A TPU
Desmopan® 3070AU TPU
Desmopan 3385A TPU
Desmopan 385E TPU
Desmopan 385S TPU
Desmopan 392 TPU
Desmopan 445 TPU
Desmopan 453 TPU
Desmopan 453 DPS041 TPU
Desmopan 460 TPU
Desmopan 481 TPU
Desmopan 487 DPS062 TPU
Desmopan 588 E TPU
Desmopan 786E TPU
Desmopan 790 TPU
Desmopan 795U TPU
Desmopan 9370A TPU
Desmopan 9370A GMP TPU
Desmopan 1050D TPU
Desmopan 3055D TPU
Desmopan 3059D TPU
Desmopan 3065D TPU
Desmopan 3072D TPU
Desmopan 5080A TPU
Desmopan 6064A TPU
Desmopan 6072A TPU
Desmopan 6080A TPU
Desmopan 85085A DPS055 TPU
Desmopan 85786A TPU
Desmopan 9370AU TPU
Desmopan 9380A TPU
Desmopan 9392A TPU
Desmopan 9662DU TPU
Desmopan 9665DU TPU
Desmopan 9855DU TPU
Desmopan 9868DU TPU
Desmopan 9873DU TPU
Desmopan 9885DU TPU
Desmopan 3055DU TPU
Desmopan 3860D (TPU+ABS)
Desmopan 588 L TPU
Desmopan® CQ2050D RC99 TPU
Desmopan® 359X DPS300 TPU
Desmopan® CQ3860D MBC091 TPU
Desmopan® 6088A TPU
Desmopan® CQ9868DU MBC091 TPU
Desmopan® CQ9873DU MBC091 TPU
Desmopan® CQ80D RC100 TPU
Desmopan® CQ385E RC50 TPU
Desmopan® CQ9385A RC050 TPU
Desmopan® CQ33375AUEC DPS300 TPU
Desmopan® 192 DPS700 TPU
Desmopan 9385 A TPU
Desmopan® CQ33085AUEC DPS300 TPU
Desmopan® CQ33095AUEC DPS300 TPU
Desmopan® CQ6088A MBC091 TPU
Desmopan 5377A TPU
Desmopan 9380AU TPU
Desmopan® CQ80D RC99 TPU
Desmopan® CQ3392A RC50 TPU
Desmopan CQ192 MBC091 TPU
Desmopan 9385AU DPS650 TPU
Desmopan 9365D TPU
Desmopan 9385D TPU
Desmopan CQ9385D MBC091 TPU

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.