Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of DuraForm® ProX® FR1200 - PA12 - 3D Systems Corporation

Material Data Center offers the following functions for DuraForm® ProX® FR1200:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Duraform datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Modulus 2006 MPa ASTM D 638
Tensile Strength 44.9 MPa ASTM D 638
Elongation at Break 8 % ASTM D 638
Flexural Modulus 1717 MPa ASTM D 790
Flexural Strength 61.4 MPa ASTM D 790
Shore D Hardness 77 - ASTM D 2240
Izod Impact notched, 1/8 in 26.7 J/m ASTM D 256
Izod Impact unnotched, 1/8 in 278 J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ISO Data
Burning behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm -
Yellow Card available yes - -
ASTM Data
UL 94 Flame rating V-2 - UL 94
Thickness tested 5.08 mm -
DTUL @ 66 psi 180 °C ASTM D 648
DTUL @ 264 psi 93.9 °C ASTM D 648
Other Standards[S]
Coefficient of Thermal Expansion, MD 137 E-6/K ASTM E 831
Specific Heat 1040 J/(kg K) ASTM E 1269
S: These properties are reported by the producer according standards that are different to our defaults.
Electrical propertiesValueUnitTest Standard
ASTM Data
Dielectric Strength, Short Time 17.4 kV/mm ASTM D 149
Surface Resistivity 1.11E13 Ohm ASTM D 257
Volume Resistivity 3.61E14 Ohm*cm ASTM D 257
Other propertiesValueUnitTest Standard
Water Absorption, Equilibrium 0.1 % ASTM D 570
Density 1030 kg/m³ ASTM D 792
Characteristics
Processing
Additive Manufacturing
Delivery form
Powder, White
Special Characteristics
Flame retardant, Halogen-free
Features
Low Smoke
Applications
Aircraft and Aerospace, Automotive, Electrical and Electronical
Regional Availability
North America, Europe, Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.