Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Dynaflex™ G7930-9 NSFG - TPE - Avient Corporation

Material Data Center offers the following functions for Dynaflex™ G7930-9 NSFG:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Dynaflex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Melt Flow Index, MFI 37 g/10min ASTM D 1238
Temperature 200 °C -
Load 5 kg -
Mold Shrinkage, MD 0.017 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ASTM Data
Modulus at 100% Elongation 0.896 MPa ASTM D 412
Modulus at 300% Elongation 0.46 MPa ASTM D 412
Shore A Hardness 30 - ASTM D 2240
Tear Strength 17.5 kN/m ASTM D 624
Compression Set , 22 hr @ 73 °F 13 % ASTM D 395
Tensile Strength at Break 3.31 MPa ASTM D 412
Elongation at Break 650 % ASTM D 412
Other propertiesValueUnitTest Standard
Density 1050 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Mold temperature 15.6 - 26.7 °C -
Zone 1 160 - 177 °C -
Zone 2 177 - 188 °C -
Zone 3 188 - 204 °C -
Nozzle temperature 188 - 204 °C -
Screw speed 25 - 75 rpm -
Injection speed 25.4 - 127 mm/s -
Back pressure 0.345 - 1.03 MPa -
Holding pressure 0.689 - 2.41 MPa -
Characteristics
Processing
Injection Molding
Delivery form
Pellets, Black
Features
Good Adhesion, Soft Feel
Certifications
Food contact, Food approval FDA 21 CFR, Drinking water contact NSF 61
Applications
General Purpose
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com