Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ECOZEN® HF002 - Copolyester - SK Chemicals

Material Data Center offers the following functions for ECOZEN® HF002:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ecozen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
ECOZEN, conceived and developed by SK Chemicals is a bio-based, heat-resistant, and transparent bio-copolyester.
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Mold Shrinkage, MD 0.0035 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ISO Data
Yield stress 59 MPa ISO 527
Yield strain 4.3 % ISO 527
Stress at break 34 MPa ISO 527
Strain at break 300 % ISO 527
Flexural modulus, 23°C 2400 MPa ISO 178
Flexural strength 79 MPa ISO 178
Izod notched impact strength, +23°C 3.7 kJ/m² ISO 180/1A
Rockwell hardness R 115 - ISO 2039-2
ASTM Data
Tensile Strength at Yield 60 MPa ASTM D 638
Tensile Strength at Break 42.2 MPa ASTM D 638
Elongation at Yield 5 % ASTM D 638
Elongation at Break 220 % ASTM D 638
Flexural Modulus 2403 MPa ASTM D 790
Flexural Strength 86.3 MPa ASTM D 790
Rockwell Hardness R 115 - ASTM D 785
Izod Impact notched, 1/8 in 65 J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 72 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 83 °C ISO 75-1/-2
ASTM Data
DTUL @ 66 psi 79 °C ASTM D 648
DTUL @ 264 psi 68 °C ASTM D 648
Optical propertiesValueUnitTest Standard
ASTM Data
Haze 1 % ASTM D 1003
Light Transmittance 86 % ASTM D 1003
Other propertiesValueUnitTest Standard
Density 1330 kg/m³ ISO 1183
Density 1330 kg/m³ ASTM D 792
Characteristics
Processing
Film Extrusion, Sheet Extrusion, Blow Molding
Special Characteristics
Heat stabilized or stable to heat, Transparent
Features
Copolymer
Chemical Resistance
General Chemical Resistance
Certifications
Contains renewable resources, RoHS compliant
Applications
Packaging
Regional Availability
North America, Europe, Asia Pacific, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.