Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Ecozen - PET, TPC - SK Global Chemicals

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Ecozen" in Material Data Center leads to the following information:

Tradename: Ecozen
Family: PET, TPC
Producer: SK Global Chemicals
56 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
ECOZEN® BS 050 TPC
ECOZEN® BS 100 TPC
ECOZEN® BS 300 TPC
ECOZEN® BS 400 TPC
ECOZEN® YA 050 TPC
ECOZEN® YA 051 TPC
ECOZEN® YA 100 TPC
ECOZEN® YA 101 TPC
ECOZEN® YA 300 TPC
ECOZEN® YA 301 TPC
ECOZEN® YA 400 TPC
ECOZEN® YA 401 TPC
ECOZEN® YF 050 TPC
ECOZEN® YF 051 TPC
ECOZEN® YF 100 TPC
ECOZEN® YF 101 TPC
ECOZEN® YF 300 TPC
ECOZEN® YF 301 TPC
ECOZEN® YF 400 TPC
ECOZEN® YF 401 TPC
ECOZEN® YH 050 TPC
ECOZEN® YH 051 TPC
ECOZEN® YH 100 TPC
ECOZEN® YH 101 TPC
ECOZEN® YH 300 TPC
ECOZEN® YH 301 TPC
ECOZEN® YH 400 TPC
ECOZEN® YH 401 TPC
ECOZEN® YM 050 TPC
ECOZEN® YM 051 TPC
ECOZEN® YM 100 TPC
ECOZEN® YM 101 TPC
ECOZEN® YM 300 TPC
ECOZEN® YM 301 TPC
ECOZEN® YM 400 TPC
ECOZEN® YM 401 TPC
ECOZEN® Claro 100 Copolyester
ECOZEN® Claro 200 Copolyester
ECOZEN® HF002 Copolyester
ECOZEN® HF502 Copolyester
ECOZEN® T90 Copolyester
ECOZEN® T90D Copolyester
ECOZEN® T90G Copolyester
ECOZEN® T90H Copolyester
ECOZEN® T95 Copolyester
ECOZEN® T95G Copolyester
ECOZEN® T110 Copolyester
ECOZEN® T110G Copolyester
ECOZEN® T120 Copolyester
ECOZEN® T120G Copolyester
ECOZEN® MT10G Copolyester
ECOZEN® Claro 300 Copolyester
ECOZEN® T110G PRO Copolyester
ECOZEN® Claro 50 Copolyester
ECOZEN® T110 Plus Copolyester
ECOZEN® T110 PRO Copolyester

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.