Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Elastollan® 1175 A W - (TPU-ARET) - BASF Polyurethanes GmbH

Material Data Center offers the following functions for Elastollan® 1175 A W:
unit conversion, PDF datasheet print, comparison with other plastics, parameters for material models, CAE Interfaces

Check here, which other Elastollan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
DESCRIPTION
Elastollan 1175 AW is a polyether based TPU with plasticiser

SPECIAL PROPERTIES
excellent resistance to hydrolysis and good flexibility at low temperature,
resistance to microbiological attack, good wear performance,
high tensile strength, good damping behavior

TYPICAL APPLICATIONS
cable sheathing, plugs and terminations, hoses, damping elements

OTHER HINTS
predrying: 2-3h at 70-85°C (dehumidified air dryer),
max. content of humidity before processing: 0,02%
annealing: 20 h at 100°C in order to get optimum properties

CHEMICAL RESISTANCE
For detailed information on the chemical resistance of our
materials refer to this list of chemical resistance
Mechanical propertiesValueUnitTest Standard
ISO Data
Stress at 50% strain 3 MPa ISO 527
Strain at break >50 % ISO 527
Stress at 100% elongation 4 MPa ISO 527
Stress at 300% elongation 8 MPa ISO 527
Stress at break TPE 40 MPa ISO 527
Strain at break TPE >300 % ISO 527
Compression set at 23 °C, 24h 20 % ISO 815
Compression set at 70 °C, 24h 40 % ISO 815
Tear strength 40 kN/m ISO 34-1
Abrasion resistance 45 mm³ ISO 4649
Shore A hardness 75 - ISO 7619-1
Thermal propertiesValueUnitTest Standard
ISO Data
Glass transition temperature, 10°C/min -46 °C ISO 11357-1/-2
Burning Behav. at 1.5 mm nom. thickn. V-2 class IEC 60695-11-10
Burning Behav. at thickness h V-0 class IEC 60695-11-10
Oxygen index 25 % ISO 4589-1/-2
Electrical propertiesValueUnitTest Standard
ISO Data
Dissipation factor, 1MHz 1100 E-4 IEC 62631-2-1
Comparative tracking index 600 - IEC 60112
Other propertiesValueUnitTest Standard
Density 1140 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 200 °C ISO 294
Injection Molding, mold temperature 60 °C ISO 294
Diagrams
Viscosity-shear rate , Elastollan® 1175 A W, (TPU-ARET), BASF PU
Shearstress-shear rate , Elastollan® 1175 A W, (TPU-ARET), BASF PU
Dynamic Shear modulus-temperature , Elastollan® 1175 A W, (TPU-ARET), BASF PU
Stress-Strain (TPE) , Elastollan® 1175 A W, (TPU-ARET), BASF PU
Characteristics
Processing
Injection Molding, Profile Extrusion
Delivery form
Pellets
Additives
Plasticizer
Regional Availability
Other text information
Injection molding
Barrel temperature : 195 - 205 °C
Melt temperature : 205 °C
Mold temperature: 25 - 40 °C
Profile extrusion
Barrel temperature : 160 - 175 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.