Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Elastollan® R 2000 - (TPU-ARES)-GF - BASF Polyurethanes GmbH

Material Data Center offers the following functions for Elastollan® R 2000:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Elastollan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
DESCRIPTION
Elastollan R 2000 is a glass fibre-reinforced TPU

SPECIAL PROPERTIES
very good impact strength, high stiffness combined with good
strain, low thermal expansion coefficient
equivalent to metal (Al), low mould shrinkage, ease of paintability

TYPICAL APPLICATIONS
technical parts, cabinets

OTHER HINTS
predrying: 2-3h at 100-120°C
(air circulating oven or dehumidified air dryer),
max. content of humidity before processing: 0,02%
annealing: 20 h at 100°C in order to get optimum properties

CHEMICAL RESISTANCE
For detailed information on the chemical resistance of our
materials refer to this list of chemical resistance
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2000 MPa ISO 527
Stress at break 65 MPa ISO 527
Strain at break 25 % ISO 527
Charpy impact strength, +23°C 140 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 110 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 40 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 10 kJ/m² ISO 179/1eA
Stress at break TPE 65 MPa ISO 527
Strain at break TPE 25 % ISO 527
Shore D hardness 67 - ISO 7619-1
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 114 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 147 °C ISO 75-1/-2
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 1MHz 5 - IEC 62631-2-1
Dissipation factor, 100Hz 320 E-4 IEC 62631-2-1
Dissipation factor, 1MHz 560 E-4 IEC 62631-2-1
Volume resistivity 1E11 Ohm*m IEC 62631-3-1
Surface resistivity >1E15 Ohm IEC 62631-3-2
Electric strength 37 kV/mm IEC 60243-1
Comparative tracking index 600 - IEC 60112
Other propertiesValueUnitTest Standard
Density 1370 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 225 °C ISO 294
Injection Molding, mold temperature 60 °C ISO 294
Diagrams
Dynamic Shear modulus-temperature , Elastollan® R 2000, (TPU-ARES)-GF, BASF PU
Stress-strain , Elastollan® R 2000, (TPU-ARES)-GF, BASF PU
Secant modulus-strain , Elastollan® R 2000, (TPU-ARES)-GF, BASF PU
Stress-strain (isochronous) 23°C, Elastollan® R 2000, (TPU-ARES)-GF, BASF PU
Creep modulus-time 23°C, Elastollan® R 2000, (TPU-ARES)-GF, BASF PU
Creep curve 23°C, Elastollan® R 2000, (TPU-ARES)-GF, BASF PU
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Regional Availability
Other text information
Injection molding
Barrel temperature : 210 - 225 °C
Melt temperature : 225 °C
Mold temperature: 25 - 70 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.