Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Elastollan® 1147 D FHF - (TPU-ARET) - BASF Polyurethanes GmbH

Material Data Center offers the following functions for Elastollan® 1147 D FHF:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Elastollan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
DESCRIPTION
Elastollan 1147 D FHF is a halogen free, flame retarded polyether based TPU

SPECIAL PROPERTIES
excellent resistance to hydrolysis and good flexibility at low temperature,
resistance to microbiological attack, good wear performance,
high tensile strength, good damping behavior

TYPICAL APPLICATIONS
cable sheathing, hoses, profiles

OTHER HINTS
predrying: 2-3h at 100-110°C,
max. content of humidity before processing: 0,02%
annealing: 20 h at 100°C in order to get optimum properties

CHEMICAL RESISTANCE
For detailed information on the chemical resistance of our
materials refer to this list of chemical resistance
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 160 MPa ISO 527
Charpy notched impact strength, +23°C N kJ/m² ISO 179/1eA
Stress at 100% elongation 9 MPa ISO 527
Stress at 300% elongation 10 MPa ISO 527
Stress at break TPE 13 MPa ISO 527
Strain at break TPE >300 % ISO 527
Compression set at 23 °C, 24h 29 % ISO 815
Compression set at 70 °C, 24h 50 % ISO 815
Tear strength 60 kN/m ISO 34-1
Abrasion resistance 54 mm³ ISO 4649
Shore A hardness 94 - ISO 7619-1
Shore D hardness 48 - ISO 7619-1
Thermal propertiesValueUnitTest Standard
ISO Data
Burning Behav. at 1.5 mm nom. thickn. V-0 class IEC 60695-11-10
Yellow Card available yes - -
Burning Behav. at thickness h V-0 class IEC 60695-11-10
Thickness tested 3.0 mm -
Yellow Card available yes - -
Other propertiesValueUnitTest Standard
Density 1270 kg/m³ ISO 1183
Diagrams
Viscosity-shear rate , Elastollan® 1147 D FHF, (TPU-ARET), BASF PU
Shearstress-shear rate , Elastollan® 1147 D FHF, (TPU-ARET), BASF PU
Dynamic Shear modulus-temperature , Elastollan® 1147 D FHF, (TPU-ARET), BASF PU
Stress-Strain (TPE) , Elastollan® 1147 D FHF, (TPU-ARET), BASF PU
Characteristics
Processing
Injection Molding, Profile Extrusion
Regional Availability
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.