Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Elix ABS M220 - ABS - Elix Polymers, S.L.

Material Data Center offers the following functions for Elix ABS M220:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Elix datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 32 cm³/10min ISO 1133
Temperature 220 °C -
Load 10 kg -
Molding shrinkage, parallel 0.6 % ISO 294-4, 2577
Molding shrinkage, normal 0.6 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2300 MPa ISO 527
Yield stress 41 MPa ISO 527
Flexural modulus, 23°C 2200 MPa ISO 178
Charpy impact strength, +23°C 100 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 80 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 18 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 11 kJ/m² ISO 179/1eA
Izod notched impact strength, +23°C 18 kJ/m² ISO 180/1A
Izod notched impact strength 12 kJ/m² ISO 180/1A
Temperature -30 °C -
Ball indentation hardness 103 MPa ISO 2039-1
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 92 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 97 °C ISO 75-1/-2
Vicat softening temperature, B 95 °C ISO 306
Coeff. of linear therm. expansion, parallel 100 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 100 E-6/K ISO 11359-1/-2
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 100Hz 2.9 - IEC 62631-2-1
Relative permittivity, 1MHz 2.9 - IEC 62631-2-1
Dissipation factor, 100Hz 73 E-4 IEC 62631-2-1
Dissipation factor, 1MHz 90 E-4 IEC 62631-2-1
Volume resistivity >1E13 Ohm*m IEC 62631-3-1
Surface resistivity >1E15 Ohm IEC 62631-3-2
Electric strength 35 kV/mm IEC 60243-1
Other propertiesValueUnitTest Standard
Density 1050 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 240 °C ISO 294
Injection Molding, mold temperature 80 °C ISO 294
Injection Molding, injection velocity 240 mm/s ISO 294
Characteristics
Processing
Injection Molding
Certifications
RoHS compliant
Applications
General Purpose
Regional Availability
Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.