Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Etoma™ ET5106 - PA6... - Polyalloy Inc.

Material Data Center offers the following functions for Etoma™ ET5106:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Etoma datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Melt Flow Index, MFI 0.7 g/10min ASTM D 1238
Temperature 250 °C -
Load 2.16 kg -
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Strength 98.1 MPa ASTM D 638
Elongation at Break 5 % ASTM D 638
Flexural Modulus 7161 MPa ASTM D 790
Flexural Strength 147 MPa ASTM D 790
Izod Impact notched, 1/8 in 58.9 J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ASTM Data
DTUL @ 66 psi 216 °C ASTM D 648
DTUL @ 264 psi 192 °C ASTM D 648
Electrical propertiesValueUnitTest Standard
ASTM Data
Surface Resistivity 10000 Ohm ASTM D 257
Other propertiesValueUnitTest Standard
Density 1440 kg/m³ ASTM D 792
Characteristics
Special Characteristics
Increased electrical conductivity, Heat stabilized or stable to heat
Regional Availability
Europe, Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.