Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Fibrolon® 3D Cork - (PLA+Copolyester)-NF - FKuR Kunststoff GmbH

Material Data Center offers the following functions for Fibrolon® 3D Cork:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Fibrolon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Biodegradable compound suitable for the production of 3D printing filaments. Contains Cork fibers.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt flow index, MFI 3.7 g/10min ISO 1133
Temperature 190 °C -
Load 2.16 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2150 MPa ISO 527
Tensile Strength 39 MPa ISO 527
Yield strain 5.4 % ISO 527
Stress at break 19 MPa ISO 527
Strain at break 18 % ISO 527
Charpy impact strength, +23°C 60 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 4.6 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 155 °C ISO 11357-1/-3
Other propertiesValueUnitTest Standard
Biobased content 75 % -
Processing Recommendation ExtrusionValueUnitTest Standard
Type of extrusion profile - -
Pre-drying - Temperature 60 °C -
Pre-drying - Time 2 - 4 h -
Processing humidity ≤0.2 % -
Feed temperature 60 °C -
Zone 1 160 °C -
Zone 2 170 °C -
Zone 3 180 °C -
Zone 4 180 °C -
Nozzle temperature 185 °C -
Characteristics
Processing
Profile Extrusion, Additive Manufacturing
Delivery form
Pellets, Brown
Certifications
Contains renewable resources, Biodegradable
Applications
Filament for 3D Printing, Toys
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com