Processing/Physical Characteristics | Value | Unit | Test Standard |
ISO Data |
Melt volume-flow rate, MVR |
4.75[1] |
cm³/10min |
ISO 1133 |
Temperature |
380 |
°C |
- |
Load |
5 |
kg |
- |
1: | Data based an semi-finished product |
Mechanical properties | Value | Unit | Test Standard |
ASTM Data |
Tensile Modulus |
3500[2] |
MPa |
ASTM D 638 |
Tensile Strength at Yield |
94.5[2] |
MPa |
ASTM D 638 |
2: | Data based on raw material |
Thermal properties | Value | Unit | Test Standard |
ASTM Data |
DTUL @ 264 psi |
157[3] |
°C |
ASTM D 648 |
3: | Data based on raw material |
Other properties | Value | Unit | Test Standard |
Density |
1290[4] |
kg/m³ |
ASTM D 792 |
4: | Data based on raw material |
Characteristics
Processing
Additive Manufacturing
Delivery form
Monofilament, Natural Color
Features
Good Adhesion, Low Odor
Chemical Resistance
General Chemical Resistance
Applications
Aircraft and Aerospace
Regional Availability
Europe
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com