Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Genestar™ GW2458HF-1 - PA9T-GF45 FR - Kuraray Co., Ltd.

Material Data Center offers the following functions for Genestar™ GW2458HF-1:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Genestar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Genestar GW2458HF-1 is a 45%GF reinforced grade for parts that require a low warpage and a high flow suitable for card connectors.

Thanks to its JEDEC MSL 1 rating (moisture sensitive level 1), this grade shows an excellent resistance to blisters.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Molding shrinkage, parallel 0.2 % ISO 294-4, 2577
Molding shrinkage, normal 0.5 % ISO 294-4, 2577
ASTM Data
Melt Flow Index, MFI 84 g/10min ASTM D 1238
Temperature 320 °C -
Load 2.16 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 16800 MPa ISO 527
Stress at break 159 MPa ISO 527
Strain at break 2.6 % ISO 527
Charpy notched impact strength, +23°C 17 kJ/m² ISO 179/1eA
ASTM Data
Tensile Strength 165 MPa ASTM D 638
Flexural Modulus 15000 MPa ASTM D 790
Flexural Strength 225 MPa ASTM D 790
Izod Impact notched, 1/8 in 125 J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 306 °C ISO 11357-1/-3
Glass transition temperature, 10°C/min 125 °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 285 °C ISO 75-1/-2
Burning Behav. at 1.5 mm nom. thickn. V-0 class IEC 60695-11-10
ASTM Data
UL 94 Flame rating V-0 - UL 94
DTUL @ 264 psi 285 °C ASTM D 648
Melting Temperature 306 °C ASTM D 3418
Glass Transition Temperature 125 °C ASTM E 1356
Electrical propertiesValueUnitTest Standard
ASTM Data
Dielectric Strength, Short Time 30 kV/mm ASTM D 149
Volume Resistivity >1E15 Ohm*cm ASTM D 257
Other propertiesValueUnitTest Standard
Water absorption 0.08 % Sim. to ISO 62
Density 1730 kg/m³ ASTM D 792
Diagrams
Stress-strain , Genestar™ GW2458HF-1, PA9T-GF45 FR, Kuraray
Secant modulus-strain , Genestar™ GW2458HF-1, PA9T-GF45 FR, Kuraray
Characteristics
Processing
Injection Molding
Special Characteristics
Flame retardant, Heat stabilized or stable to heat
Features
Low Warpage, Weldable
Regional Availability
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.