Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Geo LF 451 - PET - Selenis Portugal, S.A.

Material Data Center offers the following functions for Geo LF 451:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Geo datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Thermal propertiesValueUnitTest Standard
ASTM Data
Melting Temperature 255 °C ASTM D 3418
Other propertiesValueUnitTest Standard
Intrinsic Viscosity 1.15 dl/g -
Acetaldehyde 1 ppm -
Color L 87 - CIE
Color b 0 - CIE
Crystallinity 52 % -
Moisture Content 0.3 % -
Bulk Density 820 kg/m³ -
Processing Recommendation ExtrusionValueUnitTest Standard
Type of extrusion fiber - -
Pre-drying - Temperature 175 °C -
Pre-drying - Time 4 - 6 h -
Processing humidity ≤0.004 % -
Melt temperature 275 - 295 °C -
Characteristics
Processing
Fiber Extrusion, Other Extrusion
Delivery form
Pellets, White
Special Characteristics
Opaque
Features
Low Odor, Melt Strength, Copolymer
Chemical Resistance
General Chemical Resistance
Certifications
Food contact, Food approval 10/2011
Applications
Monofilament
Regional Availability
North America, Europe, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.