Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of GREENFLEX® ML 30 - EVAC - Versalis S.p.A

Material Data Center offers the following functions for GREENFLEX® ML 30:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Greenflex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Greenflex ML 30 is an ethylene vinyl acetate copolymer (EVA) for injection moulding and extrusion,
Parts produced with Greenflex ML 30 show good elasticity performances and good ESCR resistance.  

Applications
Gaskets, especially when food contact is required, profiles and flexible items.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 2.5 cm³/10min ISO 1133
Temperature 190 °C -
Load 2.16 kg -
Density of melt 787 kg/m³ -
Thermal conductivity of melt 0.2 W/(m K) -
Spec. heat capacity of melt 2540 J/(kg K) -
Ejection temperature 74 °C -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 90 MPa ISO 527
Shore A hardness 94 - ISO 7619-1
Shore D hardness 42 - ISO 7619-1
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 97 °C ISO 11357-1/-3
Glass transition temperature, 10°C/min 85 °C ISO 11357-1/-2
Coeff. of linear therm. expansion, parallel 125 E-6/K ISO 11359-1/-2
Electrical propertiesValueUnitTest Standard
ISO Data
Volume resistivity >1E13 Ohm*m IEC 62631-3-1
Surface resistivity >1E15 Ohm IEC 62631-3-2
Electric strength 75 kV/mm IEC 60243-1
Other propertiesValueUnitTest Standard
Density 929 kg/m³ ISO 1183
Diagrams
Viscosity-shear rate , GREENFLEX®  ML 30, EVAC, Versalis
Shearstress-shear rate , GREENFLEX®  ML 30, EVAC, Versalis
Characteristics
Processing
Injection Molding
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Other text information
Injection molding

#2

Typical processing temperature range:

    Melt temperature         150 - 210 °C

    Mold temperature          10 -  30  °C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.