Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Grilamid LV-3 ESD black - PA12-GF30 - EMS-GRIVORY | a unit of EMS-CHEMIE AG

Material Data Center offers the following functions for Grilamid LV-3 ESD black:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, cooling time calculation, CAE Interfaces

Check here, which other Grilamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Product-nomenclature: ISO16396-PA12,GF30 C,M1HRZ,C18-080

 

Product Attributes

  Hydrolysis resistant, Improved impact resistance, Improved heat resistance, Anti-static,
Improved UV resistance (outdoor use)

Markets

  Automotive
  Fuel systems
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Molding shrinkage, parallel 0.1 / * % ISO 294-4, 2577
Molding shrinkage, normal 0.8 / * % ISO 294-4, 2577
Density of melt 1080 kg/m³ -
Thermal conductivity of melt 0.26 W/(m K) -
Spec. heat capacity of melt 2200 J/(kg K) -
Eff. thermal diffusivity 1.1E-7 m²/s -
Ejection temperature 155 °C -
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 7800 / 7000 MPa ISO 527
Stress at break 125 / 110 MPa ISO 527
Strain at break 5 / 7 % ISO 527
Charpy impact strength, +23°C 85 / 80 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 70 / 65 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 15 / 15 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 10 / 10 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 178 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 160 / * °C ISO 75-1/-2
Temp. of deflection under load, 8.00 MPa 90 / * °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 50 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 120 / * E-6/K ISO 11359-1/-2
Burning Behav. at thickness h HB / * class IEC 60695-11-10
Thickness tested 0.8 / * mm -
Other propertiesdry / condUnitTest Standard
Water absorption 1.1 / * % Sim. to ISO 62
Humidity absorption 0.6 / * % Sim. to ISO 62
Density 1280 / - kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 280 °C ISO 294
Injection Molding, mold temperature 80 °C ISO 294
Injection Molding, injection velocity 300 mm/s ISO 294
Injection Molding, pressure at hold 75 MPa ISO 294
Characteristics
Processing
Injection Molding
Delivery form
Granules, Black
Special Characteristics
Anti-static, High impact or impact modified, Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Chemical Resistance
Hydrolytically Stable
Applications
Automotive
Regional Availability
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.