Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Grilamid XE 3982 natural - PA12 - EMS-GRIVORY | a unit of EMS-CHEMIE AG

Material Data Center offers the following functions for Grilamid XE 3982 natural:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Grilamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Product-nomenclature: ISO 16396-PA12-IP,,EHL,S24-002

 

Product Attributes

  Highly flexible, Improved impact resistance, Plasticised, Improved UV resistance (outdoor use)

Markets

  Electricals & Electronics
  Cables & Tubes
  Industry & Consumer goods
  Hydraulics & Pneumatics
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Molding shrinkage, parallel 0.6 / * % ISO 294-4, 2577
Molding shrinkage, normal 1.4 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus - / 195 MPa ISO 527
Stress at 50% strain - / 18 MPa ISO 527
Strain at break - / >50 % ISO 527
Charpy impact strength, +23°C - / N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C - / N kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C - / N kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C - / 10 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 170 / * °C ISO 11357-1/-3
Temp. of deflection under load, 0.45 MPa 80 / * °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 160 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 160 / * E-6/K ISO 11359-1/-2
Burning Behav. at thickness h HB / * class IEC 60695-11-10
Thickness tested 0.8 / * mm -
Electrical propertiesdry / condUnitTest Standard
ISO Data
Volume resistivity - / 1E9 Ohm*m IEC 62631-3-1
Surface resistivity * / 1E11 Ohm IEC 62631-3-2
Electric strength - / 39 kV/mm IEC 60243-1
Comparative tracking index - / 600 - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 1.2 / * % Sim. to ISO 62
Humidity absorption 0.5 / * % Sim. to ISO 62
Density 990 / - kg/m³ ISO 1183
Characteristics
Processing
Other Extrusion
Delivery form
Granules, Natural Color
Additives
Plasticizer
Special Characteristics
High impact or impact modified, Light stabilized or stable to light, U.V. stabilized or stable to weather
Applications
Electrical and Electronical
Regional Availability
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.