Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Grilon F 47 NL natural 6064 - PA6 - EMS-GRIVORY | a unit of EMS-CHEMIE AG

Material Data Center offers the following functions for Grilon F 47 NL natural 6064:
unit conversion, PDF datasheet print, comparison with other plastics, parameters for material models, CAE Interfaces

Check here, which other Grilon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Product-nomenclature: ISO 16396-PA6,,FS,S32-030N

 

Product Attributes

  High viscosity, Improved heat resistance, Barrier material, Nucleated

Markets

  Industry & Consumer goods
  Mechanical Engineering
  Packaging
  Blow moulded containers, Non oriented film, Oriented film, Tubes

Approvals

  Food Contact
  EU Requirements, FDA
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 15 / * cm³/10min ISO 1133
Temperature 275 / * °C -
Load 5 / * kg -
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus - / 750 MPa ISO 527
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 222 / * °C ISO 11357-1/-3
Optical propertiesdry / condUnitTest Standard
ISO Data
Gloss, 60° 100 / * - ISO 2813
Other propertiesdry / condUnitTest Standard
Water absorption 9 / * % Sim. to ISO 62
Humidity absorption 3 / * % Sim. to ISO 62
Density 1140 / - kg/m³ ISO 1183
Film Propertiesdry / condUnitTest Standard
ISO Data
Stress at yield, parallel 35 / * MPa ISO 527-3
Stress at yield, normal 30 / * MPa ISO 527-3
Strain at yield, parallel 15 / * % ISO 527-3
Strain at yield, normal 15 / * % ISO 527-3
Maximum strain, parallel 700 / * % ISO 527-3
Maximum strain, normal 700 / * % ISO 527-3
Elmendorf Tear resistance, parallel 10 / * N ISO 6383-2
Elmendorf Tear resistance, normal 10 / * N ISO 6383-2
Trouser Tear resistance, parallel 30 / * N/mm ISO 6383-1
Trouser Tear resistance, normal 30 / * N/mm ISO 6383-1
Dynamic coefficient of friction 0.25 / * - ISO 8295
WVTR, 23°C/85%r.h. 15 / * g/(m²*d) ISO 15106-1/-2
Oxygen transmission rate, 23°C/0%r.h. 25 / * cm³/(m²*d*bar) ISO 15105-1/-2
Oxygen transmission rate, 23°C/85%r.h. 50 / * cm³/(m²*d*bar) ISO 15105-1/-2
Carbon Dioxide transm. rate, 23°C/0%r.h. 80 / * cm³/(m²*d*bar) ISO 15105-1/-2
Carbon Dioxide transm. rate, 23°C/85%r.h. 250 / * cm³/(m²*d*bar) ISO 15105-1/-2
Diagrams
Viscosity-shear rate , Grilon F 47 NL natural 6064, PA6, EMS-GRIVORY
Shearstress-shear rate , Grilon F 47 NL natural 6064, PA6, EMS-GRIVORY
Stress-Strain (Film Grades) , Grilon F 47 NL natural 6064 (cond.), PA6, EMS-GRIVORY
Characteristics
Processing
Film Extrusion, Other Extrusion, Blow Molding
Delivery form
Granules, Natural Color
Special Characteristics
Heat stabilized or stable to heat
Features
Barrier Properties, Nucleated
Certifications
Food contact, Food approval FDA 21 CFR
Applications
Packaging
Regional Availability
Chemical Media Resistance
Acids
Acetic Acid (5% by mass) (23°C)
Citric Acid solution (10% by mass) (23°C)
Lactic Acid (10% by mass) (23°C)
Hydrochloric Acid (36% by mass) (23°C)
Nitric Acid (40% by mass) (23°C)
Sulfuric Acid (38% by mass) (23°C)
Sulfuric Acid (5% by mass) (23°C)
Chromic Acid solution (40% by mass) (23°C)
Bases
Sodium Hydroxide solution (35% by mass) (23°C)
Sodium Hydroxide solution (1% by mass) (23°C)
Ammonium Hydroxide solution (10% by mass) (23°C)
Alcohols
Isopropyl alcohol (23°C)
Methanol (23°C)
Ethanol (23°C)
Hydrocarbons
n-Hexane (23°C)
Toluene (23°C)
iso-Octane (23°C)
Ketones
Acetone (23°C)
Ethers
Diethyl ether (23°C)
Mineral oils
SAE 10W40 multigrade motor oil (23°C)
SAE 10W40 multigrade motor oil (130°C)
SAE 80/90 hypoid-gear oil (130°C)
Insulating Oil (23°C)
Standard Fuels
ISO 1817 Liquid 1 (60°C)
ISO 1817 Liquid 2 (60°C)
ISO 1817 Liquid 3 (60°C)
ISO 1817 Liquid 4 (60°C)
Standard fuel without alcohol (pref. ISO 1817 Liquid C) (23°C)
Standard fuel with alcohol (pref. ISO 1817 Liquid 4) (23°C)
Diesel fuel (pref. ISO 1817 Liquid F) (23°C)
Diesel fuel (pref. ISO 1817 Liquid F) (90°C)
Diesel fuel (pref. ISO 1817 Liquid F) (>90°C)
Salt solutions
Sodium Chloride solution (10% by mass) (23°C)
Sodium Hypochlorite solution (10% by mass) (23°C)
Sodium Carbonate solution (20% by mass) (23°C)
Sodium Carbonate solution (2% by mass) (23°C)
Zinc Chloride solution (50% by mass) (23°C)
Other
Ethyl Acetate (23°C)
Hydrogen peroxide (23°C)
DOT No. 4 Brake fluid (130°C)
Ethylene Glycol (50% by mass) in water (108°C)
1% nonylphenoxy-polyethyleneoxy ethanol in water (23°C)
50% Oleic acid + 50% Olive Oil (23°C)
Water (23°C)
Deionized water (90°C)
Phenol solution (5% by mass) (23°C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.