Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Grivory G 16 natural - PA6I/6T - EMS-GRIVORY | a unit of EMS-CHEMIE AG

Material Data Center offers the following functions for Grivory G 16 natural:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, cooling time calculation, CAE Interfaces

Check here, which other Grivory datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Product-nomenclature: ISO 16396-PA6I/6T,,FT,S09-030

 

Co Polyamide

Partially aromatic Polyamide

Product Attributes

  Highly transparent, Barrier material, Improved UV resistance (outdoor use)

Markets

  Packaging
  Paper coating, Cosmetics / Personal care

Approvals

  Food Contact
  EU Requirements, FDA
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 100 / * cm³/10min ISO 1133
Temperature 275 / * °C -
Load 5 / * kg -
Density of melt 1100 kg/m³ -
Thermal conductivity of melt 0.21 W/(m K) -
Spec. heat capacity of melt 2000 J/(kg K) -
Eff. thermal diffusivity 9.55E-8 m²/s -
Ejection temperature 120 °C -
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 3000 / 3000 MPa ISO 527
Yield stress 100 / 100 MPa ISO 527
Yield strain 5 / 5 % ISO 527
Nominal strain at break >50 / >50 % ISO 527
Charpy notched impact strength, +23°C 8 / 8 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 8 / 2 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Glass transition temperature, 10°C/min 125 / * °C ISO 11357-1/-2
Optical propertiesdry / condUnitTest Standard
ISO Data
Gloss, 60° 160 / * - ISO 2813
Other propertiesdry / condUnitTest Standard
Water absorption 7 / * % Sim. to ISO 62
Humidity absorption 2 / * % Sim. to ISO 62
Density 1180 / - kg/m³ ISO 1183
Film Propertiesdry / condUnitTest Standard
ISO Data
Stress at yield, parallel 85 / * MPa ISO 527-3
Stress at yield, normal 85 / * MPa ISO 527-3
Strain at yield, parallel 5 / * % ISO 527-3
Strain at yield, normal 5 / * % ISO 527-3
Maximum strain, parallel 200 / * % ISO 527-3
Maximum strain, normal 200 / * % ISO 527-3
Elmendorf Tear resistance, parallel 10 / * N ISO 6383-2
Elmendorf Tear resistance, normal 10 / * N ISO 6383-2
Trouser Tear resistance, parallel 5 / * N/mm ISO 6383-1
Trouser Tear resistance, normal 5 / * N/mm ISO 6383-1
WVTR, 23°C/85%r.h. 7 / * g/(m²*d) ISO 15106-1/-2
Oxygen transmission rate, 23°C/0%r.h. 30 / * cm³/(m²*d*bar) ISO 15105-1/-2
Oxygen transmission rate, 23°C/85%r.h. 10 / * cm³/(m²*d*bar) ISO 15105-1/-2
Carbon Dioxide transm. rate, 23°C/0%r.h. 90 / * cm³/(m²*d*bar) ISO 15105-1/-2
Carbon Dioxide transm. rate, 23°C/85%r.h. 40 / * cm³/(m²*d*bar) ISO 15105-1/-2
Characteristics
Processing
Injection Molding, Film Extrusion, Coating, Blow Molding
Delivery form
Granules, Natural Color
Special Characteristics
U.V. stabilized or stable to weather, Transparent
Features
Barrier Properties, Copolymer
Certifications
Food contact, Food approval FDA 21 CFR
Applications
Packaging
Regional Availability
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com