Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Grivory GV-6H black 9915 - PA*-GF60 - EMS-GRIVORY | a unit of EMS-CHEMIE AG

Material Data Center offers the following functions for Grivory GV-6H black 9915:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Grivory datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Product-nomenclature: ISO 16396-PA66 PA6I/X,GF60,M1H,C14-220

 

Partially aromatic Polyamide

Product Attributes

  Improved heat resistance

Markets

  Automotive
  Air intake sytems, Compressed air systems, Hydraulic systems,
Automotive electr. and electronics, lighting, Cooling and climate control, Powertrain and Chassis, Interior, Exterior
  Electricals & Electronics
  Electrical appliances, Electrical equipment, Connectors, Energy distribution,
Mobile phones and other portable devices, Lighting
  Industry & Consumer goods
  Housewares, Hydraulics & Pneumatics, Mechanical Engineering, Power transmission, Sports & Leisure,
Tools & Accessories

Approvals

  Potable Water Contact
  NSF 61
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Molding shrinkage, parallel 0.1 / * % ISO 294-4, 2577
Molding shrinkage, normal 0.3 / * % ISO 294-4, 2577
Density of melt 1500 kg/m³ -
Thermal conductivity of melt 0.3 W/(m K) -
Spec. heat capacity of melt 1700 J/(kg K) -
Eff. thermal diffusivity 1.18E-7 m²/s -
Ejection temperature 230 °C -
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 22000 / 21000 MPa ISO 527
Stress at break 260 / 240 MPa ISO 527
Strain at break 2 / 2 % ISO 527
Charpy impact strength, +23°C 80 / 80 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 80 / 80 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 14 / 14 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 13 / 13 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 260 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 235 / * °C ISO 75-1/-2
Temp. of deflection under load, 8.00 MPa 175 / * °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 15 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 90 / * E-6/K ISO 11359-1/-2
Burning Behav. at thickness h HB / * class IEC 60695-11-10
Thickness tested 0.8 / * mm -
Electrical propertiesdry / condUnitTest Standard
ISO Data
Volume resistivity 1E12 / 1E12 Ohm*m IEC 62631-3-1
Surface resistivity * / 1E13 Ohm IEC 62631-3-2
Electric strength 33 / 33 kV/mm IEC 60243-1
Comparative tracking index - / 600 - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 3.5 / * % Sim. to ISO 62
Humidity absorption 1.2 / * % Sim. to ISO 62
Density 1690 / - kg/m³ ISO 1183
Diagrams
Dynamic Shear modulus-temperature , Grivory GV-6H black 9915 (dry), PA*-GF60, EMS-GRIVORY
Dynamic Shear modulus-temperature , Grivory GV-6H black 9915 (cond.), PA*-GF60, EMS-GRIVORY
Stress-strain , Grivory GV-6H black 9915 (dry), PA*-GF60, EMS-GRIVORY
Stress-strain , Grivory GV-6H black 9915 (cond.), PA*-GF60, EMS-GRIVORY
Secant modulus-strain , Grivory GV-6H black 9915 (dry), PA*-GF60, EMS-GRIVORY
Secant modulus-strain , Grivory GV-6H black 9915 (cond.), PA*-GF60, EMS-GRIVORY
Stress-strain (isochronous) 80°C, Grivory GV-6H black 9915 (dry), PA*-GF60, EMS-GRIVORY
Creep modulus-time 80°C, Grivory GV-6H black 9915 (dry), PA*-GF60, EMS-GRIVORY
Creep curve 80°C, Grivory GV-6H black 9915 (dry), PA*-GF60, EMS-GRIVORY
Specific volume-temperature (pvT) , Grivory GV-6H black 9915, PA*-GF60, EMS-GRIVORY
Characteristics
Processing
Injection Molding
Delivery form
Granules, Black
Special Characteristics
Heat stabilized or stable to heat
Certifications
Drinking water contact, Drinking water contact NSF 61
Applications
Automotive, Electrical and Electronical, Sports Equipment
Regional Availability
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.