Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of HOSTAFORM® C 9021 GV3/30 - POM-GB30 - Celanese

Material Data Center offers the following functions for HOSTAFORM® C 9021 GV3/30:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Hostaform datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Chemical abbreviation according to ISO 1043-1: POM Molding compound ISO 29988- POM-K, M-GNR, 02-002, GB30 POM copolymer Injection molding type, reinforced with ca. 30 % glass spheres; high resistance to thermal and oxidative degradation. UL-registration in natural and a thickness more than 0.81 mm, in black and a thickness more than 1.0 mm as UL94 HB, temperature index UL 746 B for a thickness of 1.57 mm, electrical 105 °C, mechanical 95 °C (tensile impact) and 100 °C (tensile). Burning rate ISO 3795 and FMVSS 302 < 100 mm/min for a thickness more than 1 mm. Ranges of applications: For low-warpage and dimensionally stable molded parts with higher rigidity and hardness. FMVSS = Federal Motor Vehicle Safety Standard (USA) UL = Underwriters Laboratories (USA)

Flammability @1.6mm nom. thickn.HB-
Flammability at thickness h (0.81 mm)HBUL recognition (h)
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 7.5 cm³/10min ISO 1133
Temperature 190 °C -
Load 2.16 kg -
Molding shrinkage, parallel 1.7 % ISO 294-4, 2577
Molding shrinkage, normal 1.4 % ISO 294-4, 2577
Density of melt 1370 kg/m³ -
Thermal conductivity of melt 0.225 W/(m K) -
Spec. heat capacity of melt 1780 J/(kg K) -
Eff. thermal diffusivity 7.3E-8 m²/s -
Ejection temperature 140 °C -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 3900 MPa ISO 527
Yield stress 38 MPa ISO 527
Yield strain 6 % ISO 527
Nominal strain at break 12 % ISO 527
Charpy impact strength, +23°C 40 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 40 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 3 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 3 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 166 °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 112 °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 90 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 90 E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.6 mm -
Burning Behav. at thickness h HB class IEC 60695-11-10
Thickness tested 0.8 mm -
Yellow Card available yes - -
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 100Hz 5 - IEC 62631-2-1
Relative permittivity, 1MHz 4.5 - IEC 62631-2-1
Dissipation factor, 100Hz 300 E-4 IEC 62631-2-1
Dissipation factor, 1MHz 80 E-4 IEC 62631-2-1
Volume resistivity 1E12 Ohm*m IEC 62631-3-1
Surface resistivity 1E14 Ohm IEC 62631-3-2
Electric strength 40 kV/mm IEC 60243-1
Other propertiesValueUnitTest Standard
Water absorption 0.9 % Sim. to ISO 62
Humidity absorption 0.12 % Sim. to ISO 62
Density 1590 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 100 - 120 °C -
Pre-drying - Time 3 - 6 h -
Processing humidity ≤0.2 % -
Melt temperature 190 - 210 °C -
Mold temperature 80 - 120 °C -
Diagrams
Viscosity-shear rate , HOSTAFORM® C 9021 GV3/30, POM-GB30, Celanese
Shearstress-shear rate , HOSTAFORM® C 9021 GV3/30, POM-GB30, Celanese
Dynamic Shear modulus-temperature , HOSTAFORM® C 9021 GV3/30, POM-GB30, Celanese
Stress-strain , HOSTAFORM® C 9021 GV3/30, POM-GB30, Celanese
Secant modulus-strain , HOSTAFORM® C 9021 GV3/30, POM-GB30, Celanese
Characteristics
Processing
Injection Molding
Delivery form
Pellets, Black, Natural Color
Additives
Release agent
Features
Low Warpage, Thermal Stability, Copolymer
Chemical Resistance
Oxidation Resistance
Certifications
Drinking water contact
Applications
Automotive
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Other text information
Injection molding
General drying is not necessary due to low moisture absorption of
the resin.

In case of bad storage conditions (water contact or condensed water)
the use of a recirculating air dryer (100 to 120 °C / max. 40 mm
layer / 3 to 6 hours) is recommended.

Max. Water content 0,2 %
Standard injection moulding machines with three phase (15 to 25 D)
plasticating screws will fit.

Conditioning e.g. moisturizing is not necessary.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com