Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Hostalen GF 9055 F - (PE-HD) - LyondellBasell Industries

Material Data Center offers the following functions for Hostalen GF 9055 F:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Hostalen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt flow index, MFI 1.8 g/10min ISO 1133
Temperature 190 °C -
Load 5 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 1000 MPa ISO 527
Yield stress 27 MPa ISO 527
Yield strain 10 % ISO 527
Tensile notched impact strength, +23°C 30 kJ/m² ISO 8256/1
Shore D hardness 63 - ISO 7619-1
Thermal propertiesValueUnitTest Standard
ISO Data
Vicat softening temperature, B 80 °C ISO 306
Other propertiesValueUnitTest Standard
Density 954 kg/m³ ISO 1183
Film PropertiesValueUnitTest Standard
ISO Data
Maximum strain, parallel 430 % ISO 527-3
Elmendorf Tear resistance, parallel 0.8 N ISO 6383-2
Elmendorf Tear resistance, normal 0.2 N ISO 6383-2
Type of extrusion blown - -
Thickness of specimen 0.03 mm -
Characteristics
Processing
Blown Film Extrusion
Delivery form
Pellets
Features
Barrier Properties, Low Gel
Chemical Resistance
Oxidation Resistance
Certifications
Food contact, Food approval 1935/2004/EC, Food approval 10/2011, Food approval FDA 21 CFR
Applications
Packaging
Regional Availability
Europe
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.