Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of INNOPRENE 1800 B - TPE - Kumho Polychem

Material Data Center offers the following functions for INNOPRENE 1800 B:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Innoprene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Strength 9.81 MPa ISO 37
Compression set at 70 °C, 24h 45 % ISO 815
Tear strength 49 kN/m ISO 34-1
Shore A hardness 80 - ISO 7619-1
ASTM Data
Modulus at 100% Elongation 3.4 MPa ASTM D 412
Shore A Hardness 80 - ASTM D 2240
Tear Strength 49 kN/m ASTM D 624
Compression Set , 22 hr @ 158 °F 45 % ASTM D 395
Tensile Strength 9.81 MPa ASTM D 412
Other propertiesValueUnitTest Standard
Density 960 kg/m³ ISO 1183
Density 960 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 85 °C -
Pre-drying - Time 3 h -
Melt temperature 190 - 230 °C -
Mold temperature 10 - 60 °C -
Zone 1 160 - 180 °C -
Zone 2 180 - 200 °C -
Zone 3 200 °C -
Nozzle temperature 200 - 220 °C -
Processing Recommendation ExtrusionValueUnitTest Standard
Pre-drying - Temperature 85 °C -
Pre-drying - Time 3 h -
Melt temperature 190 - 230 °C -
Feed temperature 160 - 170 °C -
Zone 1 180 - 200 °C -
Zone 2 180 - 200 °C -
Zone 3 180 - 200 °C -
Nozzle temperature 180 - 210 °C -
Characteristics
Processing
Injection Molding, Pipe/Tube Extrusion, Profile Extrusion, Sheet Extrusion, Wire/Cable Extrusion, Blow Molding, Calandering
Delivery form
Pellets, Black
Special Characteristics
U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Features
Fatigue Resistance
Chemical Resistance
General Chemical Resistance, Ozone Resistance
Applications
General Purpose
Regional Availability
Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.