Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of IROGRAN® A 60 E 4612 N - TPU - Huntsman Polymers Corp.

Material Data Center offers the following functions for IROGRAN® A 60 E 4612 N:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Irogran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Molding shrinkage, parallel 3.0 % ISO 294-4, 2577
ASTM Data
Mold Shrinkage, MD 0.03 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ISO Data
Compression set at 23 °C, 24h 43 % ISO 815
Compression set at 70 °C, 24h 54 % ISO 815
Tear strength 35 kN/m ISO 34-1
Abrasion resistance 55 mm³ ISO 4649
ASTM Data
Modulus at 100% Elongation 3.52 MPa ASTM D 412
Modulus at 300% Elongation 5.52 MPa ASTM D 412
Shore A Hardness 65 - ASTM D 2240
Shore D Hardness 18 - ASTM D 2240
Tear Strength 63 kN/m ASTM D 624
Compression Set , 22 hr @ 158 °F 54 % ASTM D 395
Tensile Strength 25.5 MPa ASTM D 412
Elongation at Break 900 % ASTM D 412
Other propertiesValueUnitTest Standard
Density 1170 kg/m³ ISO 1183
Density 1170 kg/m³ ASTM D 792
Characteristics
Processing
Injection Molding
Regional Availability
North America, Europe, Asia Pacific, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.