Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ISOTER® A 30 200 FR V0 - ABS - Sirmax S.p.A.

Material Data Center offers the following functions for ISOTER® A 30 200 FR V0:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Isoter datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt flow index, MFI 30 g/10min ISO 1133
Temperature 220 °C -
Load 10 kg -
Molding shrinkage, parallel 0.5 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
ISO Data
Stress at break 40 MPa ISO 527
Strain at break 10 % ISO 527
Flexural modulus, 23°C 2200 MPa ISO 178
Flexural strength 63 MPa ISO 178
Charpy impact strength, +23°C 150 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 20 kJ/m² ISO 179/1eA
Izod notched impact strength, +23°C 20 kJ/m² ISO 180/1A
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 70 °C ISO 75-1/-2
Vicat softening temperature, B 86 °C ISO 306
Burning behav. at 1.5 mm nom. thickn. V-0 class IEC 60695-11-10
Thickness tested 1.5 mm -
Yellow Card available yes - -
Glow Wire Flammability Index (GWFI) 850 °C IEC 60695-2-12
GWFI - thickness tested (1) 1 mm -
Glow Wire Flammability Index (GWFI) 850 °C IEC 60695-2-12
GWFI - thickness tested (2) 3 mm -
Electrical propertiesValueUnitTest Standard
ISO Data
Volume resistivity 1E16 Ohm*m IEC 62631-3-1
Surface resistivity 1E16 Ohm IEC 62631-3-2
Other propertiesValueUnitTest Standard
Density 1200 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 70 - 80 °C -
Pre-drying - Time 0.5 - 2 h -
Melt temperature 200 - 230 °C -
Mold temperature 60 - 80 °C -
Characteristics
Processing
Injection Molding
Special Characteristics
Flame retardant
Certifications
RoHS compliant
Applications
Electrical and Electronical
Regional Availability
North America, Europe, Asia Pacific, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.