Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ISPLEN® PM440 AT - PP-MX40 - Repsol YPF S.A.

Material Data Center offers the following functions for ISPLEN® PM440 AT:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Isplen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt flow index, MFI 3 g/10min ISO 1133
Temperature 230 °C -
Load 2.16 kg -
Molding shrinkage, parallel 0.7 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 4300 MPa ISO 527
Yield stress 32 MPa ISO 527
Yield strain 3 % ISO 527
Flexural modulus, 23°C 4550 MPa ISO 178
Izod impact strength, +23°C 17.5 kJ/m² ISO 180/1U
Izod notched impact strength, +23°C 2.9 kJ/m² ISO 180/1A
Izod notched impact strength 2.8 kJ/m² ISO 180/1A
Shore D hardness 77 - ISO 7619-1
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 79 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 124 °C ISO 75-1/-2
Vicat softening temperature, A 156 °C ISO 306
Vicat softening temperature, B 107 °C ISO 306
Other propertiesValueUnitTest Standard
Density 1230 kg/m³ ISO 1183
Characteristics
Special Characteristics
Heat stabilized or stable to heat
Features
Low Warpage, Homopolymer
Chemical Resistance
General Chemical Resistance
Applications
Automotive, Electrical and Electronical
Regional Availability
North America, Europe, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com