Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Iupiace GN10 - (PPE+PS)-GF10 - Mitsubishi Engineering-Plastics Corporation

Material Data Center offers the following functions for Iupiace GN10:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Iupiace datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 7 cm³/10min ISO 1133
Temperature 300 °C -
Load 2.16 kg -
Molding shrinkage, parallel 0.3 % ISO 294-4, 2577
Molding shrinkage, normal 0.4 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 4200 MPa ISO 527
Stress at break 83 MPa ISO 527
Strain at break 2.5 % ISO 527
Flexural modulus, 23°C 4000 MPa ISO 178
Flexural strength 140 MPa ISO 178
Charpy notched impact strength, +23°C 7 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 125 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 130 °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 45 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 75 E-6/K ISO 11359-1/-2
Burning behav. at thickness h V-0 class IEC 60695-11-10
Thickness tested 0.8 mm -
Yellow Card available yes - -
Burning behav. 5V at thickness h 5VA class IEC 60695-11-20
Thickness tested 2.0 mm -
Yellow Card available yes - -
Electrical propertiesValueUnitTest Standard
ISO Data
Volume resistivity 3E14 Ohm*m IEC 62631-3-1
Surface resistivity 2E15 Ohm IEC 62631-3-2
Comparative tracking index 200 - IEC 60112
Other propertiesValueUnitTest Standard
Water absorption 0.06 % Sim. to ISO 62
Density 1170 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 100 - 120 °C -
Pre-drying - Time 2 - 4 h -
Mold temperature 90 - 125 °C -
Zone 1 260 - 290 °C -
Zone 2 280 - 310 °C -
Zone 3 280 - 310 °C -
Nozzle temperature 270 - 310 °C -
Screw speed 60 - 150 rpm -
Injection pressure 20 - 150 MPa -
Characteristics
Processing
Injection Molding
Special Characteristics
Flame retardant
Applications
Automotive, Electrical and Electronical, General Purpose
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.