Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Iupital F25-03 - POM - Mitsubishi Engineering-Plastics Corporation

Material Data Center offers the following functions for Iupital F25-03:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Iupital datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 14 cm³/10min ISO 1133
Temperature 190 °C -
Load 2.16 kg -
Melt flow index, MFI 16 g/10min ISO 1133
Temperature 190 °C -
Load 2.16 kg -
Molding shrinkage, parallel 2.0 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2900 MPa ISO 527
Yield stress 64 MPa ISO 527
Yield strain 8 % ISO 527
Strain at break 27 % ISO 527
Flexural modulus, 23°C 2600 MPa ISO 178
Flexural strength 90 MPa ISO 178
Charpy impact strength, +23°C 200 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 6.5 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 166 °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 100 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 156 °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 110 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 110 E-6/K ISO 11359-1/-2
Burning behav. at thickness h HB class IEC 60695-11-10
Thickness tested 0.8 mm -
Yellow Card available yes - -
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 1MHz 3.9 - IEC 62631-2-1
Dissipation factor, 1MHz 70 E-4 IEC 62631-2-1
Volume resistivity 1E12 Ohm*m IEC 62631-3-1
Surface resistivity 1E16 Ohm IEC 62631-3-2
Electric strength 32 kV/mm IEC 60243-1
Comparative tracking index 600 - IEC 60112
Other propertiesValueUnitTest Standard
Humidity absorption 0.22 % Sim. to ISO 62
Density 1410 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 °C -
Pre-drying - Time 3 - 4 h -
Mold temperature 60 - 80 °C -
Zone 1 170 °C -
Zone 2 180 °C -
Zone 3 190 °C -
Nozzle temperature 180 - 210 °C -
Screw speed 80 - 120 rpm -
Injection pressure 50 - 100 MPa -
Characteristics
Processing
Injection Molding
Features
Copolymer
Applications
Automotive, Electrical and Electronical, General Purpose
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.