Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of K-Resin® KR03E - SB - INEOS Styrolution

Material Data Center offers the following functions for K-Resin® KR03E:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, cooling time calculation, CAE Interfaces

Check here, which other K-Resin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
K-Resin® KR03E processes very well in injection molding, providing good cycle times and design flexibility. K-Resin® KR03E alone or in blends, can be extruded into sheet and thermoformed on conventional equipment at high output rates. The favorable economics of K-Resin® SBC, along with high productivity, have made possible tough clear disposable drinking cups, lids and other packaging applications. K-Resin® KR03E will process on most conventional equipment, allowing the molder to run a crystal clear bottle without expensive machine modifications, special molds, different screws, or dryers. K-Resin® KR03 can be blow molded in a broad range of sizes and shapes, from small pill bottles and medical drainage units, to very tall display bottles. It also can be injection blow molded into extremely high impact bottles with glass-like clarity.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 7.5 cm³/10min ISO 1133
Temperature 200 °C -
Load 5 kg -
Melt flow index, MFI 7.5 g/10min ISO 1133
Temperature 200 °C -
Load 5 kg -
Molding shrinkage, parallel 0.7 % ISO 294-4, 2577
Density of melt 907 kg/m³ -
Thermal conductivity of melt 0.184 W/(m K) -
Spec. heat capacity of melt 2300 J/(kg K) -
Ejection temperature 60 °C -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 1500 MPa ISO 527
Yield stress 25 MPa ISO 527
Yield strain 2.2 % ISO 527
Nominal strain at break >50 % ISO 527
Flexural modulus, 23°C 1400 MPa ISO 178
Flexural strength 30 MPa ISO 178
Charpy impact strength, +23°C N kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 2 kJ/m² ISO 179/1eA
Shore D hardness 63 - ISO 7619-1
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 61 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 76 °C ISO 75-1/-2
Vicat softening temperature, A 88 °C ISO 306
Vicat softening temperature, B 60 °C ISO 306
Optical propertiesValueUnitTest Standard
ASTM Data
Haze 1.5 % ASTM D 1003
Light Transmittance 91 % ASTM D 1003
Other propertiesValueUnitTest Standard
Humidity absorption 0.07 % Sim. to ISO 62
Density 1010 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 50 °C -
Pre-drying - Time 3 - 4 h -
Melt temperature 180 - 240 °C -
Mold temperature 30 - 50 °C -
Characteristics
Processing
Injection Molding, Sheet Extrusion, Blow Molding, Thermoforming
Delivery form
Pellets
Special Characteristics
High impact or impact modified, Transparent
Features
Blending Resin, High Gloss, Copolymer
Certifications
Food contact
Applications
IT / Business Machine, Medical, Packaging, Toys
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Other text information
Injection molding
As a rule, the K-Resin® granules do not have to be pre-dried. However, in the event of unfavorable storage or transportation conditions involving severe temperature fluctuations, moisture can condense on the surface of the granules and this then has to be removed in a pre-drying step. The granules should be pre-dried in a dry-air dryer for 3 to 4 hours at a temperature of about 50°C.

PROCESSING

Melt temperature, range: 180 - 240°C

Mold temperature, range: 30 - 50°C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.