Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of KOPEL® KP3355HR - TPE - Kolon Industries

Material Data Center offers the following functions for KOPEL® KP3355HR:
unit conversion, PDF datasheet print

Check here, which other Kopel datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt flow index, MFI 16 g/10min ISO 1133
Temperature 220 °C -
Load 2.16 kg -
Molding shrinkage, parallel 1.2 % ISO 294-4, 2577
Molding shrinkage, normal 1.2 % ISO 294-4, 2577
ASTM Data
Melt Flow Index, MFI 13.5 g/10min ASTM D 1238
Temperature 220 °C -
Load 2.16 kg -
Mold Shrinkage, MD 0.012 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Strength 32 MPa ISO 527
Flexural modulus, 23°C 161 MPa ISO 178
Charpy notched impact strength, +23°C N kJ/m² ISO 179/1eA
Shore D hardness 49 - ISO 7619-1
ASTM Data
Tensile Strength 29 MPa ASTM D 638
Flexural Modulus 211 MPa ASTM D 790
Shore D Hardness 55 - ASTM D 2240
Taber Abrasion Resistance 5 mg/1000 cycles ASTM D 1044
Izod Impact notched, 1/8 in N J/m ASTM D 256
Izod Impact notched, Low-Temperature N J/m ASTM D 256
Temperature -40 °C -
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 200 °C ISO 11357-1/-3
Vicat softening temperature, A 169 °C ISO 306
ASTM Data
UL 94 Flame rating HB - UL 94
Thickness tested 0.8 mm -
DTUL @ 66 psi 65 °C ASTM D 648
Melting Temperature 195 °C ASTM D 3418
Electrical propertiesValueUnitTest Standard
ISO Data
Volume resistivity 1E13 Ohm*m IEC 62631-3-1
Electric strength 18.8 kV/mm IEC 60243-1
Other propertiesValueUnitTest Standard
Density 1180 kg/m³ ISO 1183
Density 1200 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 100 - 120 °C -
Pre-drying - Time 3 - 6 h -
Processing humidity ≤0.08 % -
Mold temperature 30 - 80 °C -
Zone 1 160 - 190 °C -
Zone 2 160 - 210 °C -
Zone 3 180 - 220 °C -
Nozzle temperature 190 - 230 °C -
Characteristics
Processing
Injection Molding, Other Extrusion
Regional Availability
North America, Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.