Complete Set of CAMPUSĀ® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Krutene - PE-HD, PE-LD - Steinbeis PolyVert GmbH

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Krutene" in Material Data Center leads to the following information:

Tradename: Krutene
Family: PE-HD, PE-LD
Producer: Steinbeis PolyVert GmbH
21 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
Krutene-HD HDPE Pellets black MFR 0,4-1,0 / 5kg (PE-HD)
Krutene-HD HDPE Pellets black MFR 0,1-0,3 (PE-HD)
Krutene-HD HDPE Pellets black MFR 0,4-1,0 (PE-HD)
Krutene-HD HDPE Pellets blue MFR 0,1-0,3 (PE-HD)
Krutene-HD HDPE Pellets blue MFR 0,4-1,0 (PE-HD)
Krutene-HD HDPE Pellets natural MFR 5,1-8,0 (PE-HD)
Krutene-HD HDPE Pellets natural MFR 8,1-12,0 (PE-HD)
Krutene-HD HDPE Pellets natural MFR 12,1-20,0 (PE-HD)
Krutene-HD HDPE Pellets natural MFR 20,1-30,0 (PE-HD)
Krutene-LD LDPE Pellets black MFR 0,1-0,3 (PE-LD)
Krutene-LD LDPE Pellets black MFR 0,4-1,0 (PE-LD)
Krutene-LD LDPE Pellets black MFR 1,1-2,0 (PE-LD)
Krutene-LD LDPE Pellets black MFR 2,1-3,0 (PE-LD)
Krutene-LD LDPE Pellets blue MFR 0,4-1,0 (PE-LD)
Krutene-LD LDPE Pellets multi-coloured MFR 0,4-1,0 (PE-LD)
Krutene-LD LDPE Pellets natural MFR 0,4-1,0 (PE-LD)
Krutene-LD LDPE Pellets natural MFR 1,1-2,0 (PE-LD)
Krutene-LD LDPE Pellets natural MFR 2,1-3,0 (PE-LD)
Krutene-LD LDPE Pellets natural MFR 2,1-4,0 (PE-LD)
Krutene-LD LDPE Pellets natural MFR 3,1-5,0 (PE-LD)
Krutene-MD MDPE Pellets natural MFR 2,1-3,0 (PE-MD)

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.