Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kurarity™ LA2270 - TPE - Kuraray Co., Ltd.

Material Data Center offers the following functions for Kurarity™ LA2270:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kurarity datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
KURARITY is non-crystalline block copolymer and does not have melting point.
All the KURARITY grades show similar low temperature properties which result from Tg of poly (n-butyl acrylate) or poly (n-butyl acrylate/2-ethylhexyl acrylate) and heat resistance from Tg of PMMA.
LA series : n-butyl acrylate based block copolymers.
Suitable Applications: For Molding, Compound, Additives.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt flow index, MFI 4.8 g/10min ISO 1133
Temperature 190 °C -
Load 2.16 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Charpy notched impact strength, +23°C N kJ/m² ISO 179/1eA
Tensile Strength 15 MPa ISO 37
Shore A hardness 68 - ISO 7619-1
Shore D hardness 22 - ISO 7619-1
Other Standards[S]
Stress at 100% elongation 9.3 MPa ISO 37
S: These properties are reported by the producer according standards that are different to our defaults.
Thermal propertiesValueUnitTest Standard
Other Standards[S]
Thermal Conductivity, solid state 0.15 W/(m K) ASTM E 1530
S: These properties are reported by the producer according standards that are different to our defaults.
Electrical propertiesValueUnitTest Standard
Other Standards[S]
Dissipation Factor, 60 Hz 0.0288 - JIS C 2138
Dissipation Factor, 1 MHz 0.0552 - JIS C 2138
Dielectric Constant, 60 Hz 4.84 - JIS C 2138
Dielectric Constant, 1 MHz 3.97 - JIS C 2138
S: These properties are reported by the producer according standards that are different to our defaults.
Optical propertiesValueUnitTest Standard
ISO Data
Haze 2 - ISO 14782
Other Standards[S]
Light Transmittance 93 % ISO 13468-1
S: These properties are reported by the producer according standards that are different to our defaults.
Other propertiesValueUnitTest Standard
Density 1100 kg/m³ ISO 1183
Processing Recommendation ExtrusionValueUnitTest Standard
Feed temperature 100 - 130 °C -
Zone 1 140 - 160 °C -
Zone 2 150 - 170 °C -
Nozzle temperature 150 - 170 °C -
Characteristics
Processing
Other Extrusion
Delivery form
Pellets
Special Characteristics
U.V. stabilized or stable to weather, Transparent
Features
Blending Resin, Low Odor, Copolymer
Chemical Resistance
Acid Resistance, Alkali Resistance, Oil Resistance
Applications
Automotive, Electrical and Electronical
Regional Availability
North America, Europe, Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.