Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LEONA™ MR001 - PA66-MF40 - Asahi Kasei

Material Data Center offers the following functions for LEONA™ MR001:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Leona datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 5900 / 3400 MPa ISO 527
Stress at break 93 / 58 MPa ISO 527
Strain at break 5.5 / 19 % ISO 527
Flexural modulus, 23°C 5800 / 3100 MPa ISO 178
Flexural strength 150 / 84 MPa ISO 178
Charpy impact strength, +23°C 62 / 125 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 3 / 3 kJ/m² ISO 179/1eA
Rockwell hardness R 120 - ISO 2039-2
ASTM Data
Tensile Strength 98 / 67 MPa ASTM D 638
Elongation at Break 6 / 7 % ASTM D 638
Flexural Modulus 5600 / 3300 MPa ASTM D 790
Flexural Strength 157 / 98 MPa ASTM D 790
Rockwell Hardness M 85 / M 60 - ASTM D 785
Izod Impact notched, 1/8 in 34 / 39 J/m ASTM D 256
Thermal propertiesdry / condUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 118 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 229 / * °C ISO 75-1/-2
Burning Behav. at thickness h HB / * class IEC 60695-11-10
Thickness tested 0.8 / * mm -
Yellow Card available yes / * - -
ASTM Data
UL 94 Flame rating HB - UL 94
Thickness tested 0.75 mm -
Coefficient of Thermal Expansion, MD 60 E-6/K ASTM D 696
DTUL @ 66 psi 240 °C ASTM D 648
DTUL @ 264 psi 160 °C ASTM D 648
Electrical propertiesdry / condUnitTest Standard
ISO Data
Volume resistivity 1E12 / - Ohm*m IEC 62631-3-1
Surface resistivity * / 1E13 Ohm IEC 62631-3-2
Electric strength 22 / - kV/mm IEC 60243-1
ASTM Data
Dielectric Strength, Short Time 22 / - kV/mm ASTM D 149
Volume Resistivity 1E14 / - Ohm*cm ASTM D 257
Other propertiesdry / condUnitTest Standard
Humidity absorption 1.5 / * % Sim. to ISO 62
Density 1520 / - kg/m³ ISO 1183
Density 1520 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 - 90 °C -
Pre-drying - Time 2 - 3 h -
Melt temperature 275 - 295 °C -
Mold temperature 75 - 85 °C -
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Special Characteristics
Heat stabilized or stable to heat
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com